Gabriela, I do know of BGA manufactures using a SAC105 and other SAC alloys.
The reason they are doing so is for shock reliability. The SAC105 out
performs the SAC305 in shock tests. You shouldn't have any difficulty using
this alloy with your leaded paste. It should be relatively the same as a
SAC305 BGA with better performance.
Christopher J. Nash
Mid-West Technical Support Engineer
Indium Corporation of America
Phone #: (315) 853-4900 x7521
Fax #: (315) 853-1000
www.indium.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gabriela Bogdan
Sent: Friday, March 30, 2007 7:18 AM
To: [log in to unmask]
Subject: [TN] Alternative SAC
Dear Technetters:
Do you know if SnAg1Cu0.5 alloy is being used by BGA manufacturers instead
of SAC 305?
If so, what impact does it have on the mixed assembly solder profiles?
We use a peak temperature of 232C on the lead free BGA top, for lead free
BGA's on leaded solder paste on mixed assemblies.
Is the information usually available on the data sheets?
(Yesterday....)
Gaby
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|