Ryan, to my eye, it is curious that of 45 measurements, with a Cpk of
0.65, none were out of spec. My quick and perhaps erroneous calculation
suggests you could expect 2 or more of the 45 measurements to be out of
spec. It looks to me like the supplier's process is not so good, and he is
doing a 100% screen of product before shipping it to you. The distribution
of data may be like that of a normal, with the tails truncated.
Lou
Louis Hart
Technology Transfer Specialist
National Technology Transfer Center
316 Washington Av
Wheeling, WV 26003
304-243-2553
[log in to unmask]
Ryan Grant <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
03/28/2007 11:39 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
[TN] Explanation of Cpk (Ppk)
Hi all,
I have a supplier that is wondering why we rejected a shipment for
finding a critical dimension as having a Cpk of 0.65 (Ok, technically,
we are calculating Ppk). None of the 45 measurements were actually out
of spec (although one measurement just missed exceeding the upper limit
by 0.002mm). Now they want to know why we are rejecting for low Cpk.
Sigh...
Rather than go through the tedium of carefully explaining what a
distribution is, what it means, how to calculate it and what the
calculation implies, etc., does anyone know of some websites I can point
them to that can explain this?
Any help is appreciated.
Thanks,
Ryan Grant
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|