Another sceptic..me
we consider to start sample tests on many incoming parts. We have bought a
balance.
Inge
----- Original Message -----
From: "Mike Fenner" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, March 23, 2007 1:23 PM
Subject: Re: [TN] ROHS lead free question
> My advise would be to be sceptical rather than hopeful.
> If it says lead free it [probably] has a lead free finish, but need not
> have
> a ROHS compliant content.
> Just because it has no lead it doesn't mean that is capable of being
> processed to lead free temperatures.
>
> I would get a statement saying ROHS compliant and lead free processable
> before committing.
>
>
> Regards
>
> Mike Fenner
> Indium Corporation
>
> T: + 44 1908 580 400
> M: + 44 7810 526 317
> F: + 44 1908 580 411
> E: [log in to unmask]
> W: www.indium.com
> Pb-free: www.Pb-Free.com
>
> ---------------------
>
> Indium Corporation
> Incorporated in New York, USA
> Registered office: (Not for correspondence)
> 77-97 Harpur Street, Bedford , UK
> Registered number: fc16473
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of David Harman
> Sent: Friday, March 23, 2007 12:04 AM
> To: [log in to unmask]
> Subject: [TN] ROHS lead free question
>
> We are having a discussion about off -shelve- components being lead
> free.
>
> Data sheets are not specifying ROHS, however; they specify lead-free.
> Can these parts be used in a ROHS environment, and be certified as
> ROHS.?
>
>
>
>
> David Harman
> 408-790-4170 (Badge)
> 20600 Lazaneo Drive,
> Cupertino, 95014
>
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
> ***This email, its content and any files transmitted with it are intended
> solely for the addressee(s) and may be legally privileged and/or
> confidential. If you are not the intended recipient please delete and
> contact the sender by return and delete the material from any computer.
> Any review, retransmission, dissemination or other use of, or taking of
> any action in reliance upon, this information by persons or entities other
> than the intended recipient is prohibited.
>
> Messages sent via this medium may be subject to delays, non-delivery and
> unauthorized alteration. This email has been prepared using information
> believed by the author to be reliable and accurate, but Indium Corporation
> makes no warranty as to accuracy or completeness. In particular, Indium
> Corporation does not accept responsibility for changes made to this email
> after it was sent. Any opinions or recommendations expressed herein are
> solely those of the author. They may be subject to change without
> notice.***
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|