Jim
Upon reconsidering, I don't believe the Ablefilm 550 will hold up well
at 200C. Continuously at that temp it will degrade. Ablestik "K"
suffix is thermally conductive, "ECF" is electrically conductive film,
and no suffix is an unfilled mechanical resin.
Be sure to ask both for materials capable of meeting your sustained high
temp requirements.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Marsico, James
Sent: Thursday, March 22, 2007 2:26 PM
To: [log in to unmask]
Subject: [TN] structural adhesive
Hello Technet:
I'm looking for a structural adhesive, preferably available in prepreg
form, which has high bond strength and has a service temperature of
about 400 degrees F. Oh yea, also that can be purchased in a relatively
small quantity. (I'll also consider paste adhesives.)
Thanks,
Jim Marsico
EDO Corporation
Amityville: 631-630-5079
Bohemia: 631-218-7057
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|