That's something else! You did not tell what purpose. It's right, for
some multiGHZ bands, where low losses are wanted, we don't use nickel
plating because it's higher resistivity. Some nickel platings can have
10 times higher losses than Copper and Gold! In these cases, we use just
copper (no plating at all)if it's possible in environmental point of
view, or we use tinned copper lines. So, silver over copper is
theoretically right. And metallurgically spoken, silver on copper has
been used for centuries. What I don't understand is why add gold. Maybe
to avoid silver tarnish, if the package is not hermetic.
Resistivity microOhm x cm :
Electronic solder 17-20
Pure Tin 9-11
Electroless nickel 50-100
Electrolytic nickel 8-10
Electrolytic Gold 2.5
Copper lines 1.8
Electrolytic Silver 1.6
When you look at the above table, you will understand why Silver.
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tan, Geok Ang
Sent: den 19 mars 2007 14:28
To: [log in to unmask]
Subject: Re: [TN] "Greenish colour on traces"
This product is used in Microwave products, not micro-oven. Believed it
is due to the signal frequencies.
Best Regards
Geok Ang
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, March 19, 2007 8:31 PM
To: [log in to unmask]
Subject: Re: [TN] "Greenish colour on traces"
Geok
Any clue as to why someone wanted it plated this way? I think you are
having problems because your specification is incorrect.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tan, Geok Ang
Sent: Sunday, March 18, 2007 2:49 AM
To: [log in to unmask]
Subject: Re: [TN] "Greenish colour on traces"
Accordingly to the specification it is copper-silver-gold plated.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dennis Fritz
Sent: Sunday, March 18, 2007 7:44 AM
To: [log in to unmask]
Subject: Re: [TN] "Greenish colour on traces"
In a message dated 3/17/2007 8:07:29 A.M. Eastern Daylight Time,
[log in to unmask] writes:
The trace is copper-silver-gold plated.
Are you sure it is not copper nickel gold? I don't think silver is used
between copper and gold.
Nickel salts are green. Copper corrosion can look green-blue.
************************************** AOL now offers free email to
everyone.
Find out more about what's free from AOL at http://www.aol.com.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|