TECHNET Archives

March 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Clayton @ Reliability Resources" <[log in to unmask]>
Date:
Fri, 16 Mar 2007 14:11:39 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, al shirazi <[log in to unmask]>
Subject:
From:
al shirazi <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
<001401c7680d$895e4a30$2701a8c0@rresources>
Content-Type:
text/plain; charset=iso-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (81 lines)
I am still wondering if there is any hope that we can define the stress-strain of the solder joints under the thermal cycling.
   
  Let me know if you have any info.
   
  Al
  

"Clayton @ Reliability Resources" <[log in to unmask]> wrote:
  Reuven and all,
HASS is not a good tool for finding Solder Joint Failure. However, Dell,
Airbus, Thales, GM, Cisco, McData, L-3, Boeing and many others, including
several branches of the US and Canadian military, feel that HASS is a very
effective screening tool, if used correctly. HASS does not make a lousy
screening procedure. A word of caution, the terms HALT and HASS have been
widely interpreted by many companies and this has lead to misunderstandings
and poor results.

Clayton Bonn
Reliability Resources
e-mail:[log in to unmask] 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Friday, March 16, 2007 1:04 PM
To: [log in to unmask]
Subject: Re: [TN] SMT Solder Joint Strength

Hi Reuven,
You certainly would not want to do 'HASS' on product to be shipped. Saying "
after all the visual and X Ray inspections" implies product. HASS makes for
a lousy screening procedure.
The tests I recommend depend on what you try to accomplish--HASS is not
among them.

Werner



**************************************
AOL now offers free email to everyone. 
Find out more about what's free from AOL at http://www.aol.com.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


 
---------------------------------
Don't get soaked.  Take a quick peek at the forecast 
 with theYahoo! Search weather shortcut.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2