From what info I was fed by the laminate manufacturer, Isola 410 was the
material of choice for RoHS applications. To date I do not believe we
have seen any issues with this material due to wave or reflow. We have
seen other issues, but they were due to our own process not the heat of
wave or reflow.
I think this directly crosses to Polyclad 370 HR.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: Monday, March 12, 2007 12:46 PM
To: [log in to unmask]
Subject: Re: [TN] Laminate material selection
IMHO and having assessed many, many things given the known variables and
needed process controls or the lack there-of, I would only use the
following:
* Polyclad 370 HR
* Panasonic R-1755
* Nelco N4000-29
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Marsico, James
Sent: Monday, March 12, 2007 5:31 AM
To: [log in to unmask]
Subject: [TN] Laminate material selection
Hello Technet:
Can anyone provide the pros and cons with using Nelco N4000-13EP vs.
Isola FR408 with regard to PWB processing, reliability and performance
for a high reliability application? How would these compare with a
polyimide material?
Thanks in advance,
Jim Marsico
EDO Corporation
1250 New Horizons Blvd.
North Amityville, NY 11701
631-630-5079
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|