We currently use Techspray "Wondermask P". It does not have the nasty
ammonia smell of our old mask material.
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bloomquist, Ken
Sent: Friday, February 02, 2007 12:06 PM
To: [log in to unmask]
Subject: [TN] Latex Peelable Soldermask
Happy Friday TechNetters,
We currently us Latex Peelable Soldermask for temporary masking during
conformal coating. We us the HB (Heavy Body) type but the manufacturer
says they no longer make it; they only make the thinner material which
runs too much for application.
I'm curious as to what peelable materials others of you are using for
this application.
Thanks and have a Great Weekend!
KennyB
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|