Read IPC-4553, the spec for IAg fabricated boards. It has a wealth of
good information on how to handle, package, and store IAg-finished PWBs.
Also, go to MacDermid's and Cookson's websites and look at the multitude
of information for Sterling and AlphLevel finishes. There are a lot of
good papers on the same topics.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Craig Sullivan
Sent: Thursday, February 22, 2007 9:25 AM
To: [log in to unmask]
Subject: [TN] Immersion silver handling
Good morning,
Being relatively new to the Assembly process, I was wondering if any of
you could share your thoughts on handling, cleaning, processing, etc. of
assembling PWBs with Immersion Ag surface finishes. What are some
important items to watch out for? What is considered taboo when handling
these PWBs?
What is considered a must when handling, cleaning, etc.?
Searching the net yields some excellent results and reading material,
but it's always nice to hear some things first hand and from individuals
that may deal with this every day.
I appreciate everyone's time.
Regards,
Craig Sullivan
Manufacturing Engineer
MPL Incorporated
607.266.0480 Ext #32
[log in to unmask]
www.mplinc.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|