TECHNET Archives

February 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Date:
Wed, 21 Feb 2007 13:26:00 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Dave Seymour <[log in to unmask]>
Subject:
From:
Dave Seymour <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-1; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (109 lines)
Our company has been successfully using CPCI style connectors in a .250 
inch backplane
that actually insert from opposite sides of the board and share the same 
hole.
The pin length is approx. 070 inch.

The main issue is correct hole design for the press-fit pin one is using.
And as mentioned below, finding any pins that buckle during the inserting.

In circuit testing on 100% of the pins is required.

Hope this helps.

Dave



Wayne Thayer wrote:

>Only thing I see is that without full protrusion they are difficult to inspect for buckling.  Buckling is the nemesis of press-fits.  You can still inspect by looking carefully down all of the holes--0.088 doesn't sound like a very thick board, so the tips should be readily visible.  In that case, the inspection concern would be minimal.
>
>Wayne Thayer
>
>  
>
>>>>[log in to unmask] 2/21/2007 11:33 am >>>
>>>>        
>>>>
>Not sure what the question is, but if the connector is press-fit, what is
>the concern of zero or negative lead protrusion?  On the dynamic pin makes
>contact with the PTH, it is contacting all layers connected to the PTH.  So
>unless you need to solder to the tails, what's the worry?
> 
>
>-----Original Message-----
>From: Bremer, Gary [mailto:[log in to unmask]] 
>Sent: Wednesday, February 21, 2007 10:52 AM
>To: [log in to unmask] 
>Subject: [TN] Lead Protrusion
>
>Hello
>
> 
>
>We build class 3 products and engineering has allowed the tolerances to give
>me zero lead protrusion on press fit connectors and they are just now
>concerened that there might be a problem. Our board contains 10 layer and
>thickness is .088 the copper is 2 oz on all layers and for the connector the
>contacts ar .104±.010.
>
> 
>
>Steve would you post the attached pictures so other can view.
>
> 
>
>Gary Bremer
>Senior Manufacturing Engineer, CIT, CID
>  
>Curtiss-Wright Controls Inc. 
>Embedded Computing -Subsystem
>
>28965 Avenue Penn
>Santa Clarita, CA 91355-4185
>Main: 661.257.4430 extension 2170
>Fax: 661.257.4782
>
>
>e-mail: [log in to unmask] 
>Web: www.cwcembedded.com 
>
>
>  
>

-- 
Dave Seymour, CID+
Catapult Communications Inc.
800 Perimeter Park Dr, Suite A
Morrisville, NC 27560

Direct: (919)653-4249
Main: (919)653-4180
Fax: (919)653-4297

[log in to unmask]




*************************************************************
"This e-mail (and any attachments) may contain confidential and
privileged information. If you are not the intended recipient, please
notify the sender immediately by return e-mail, delete this e-mail and
destroy any copies.  Any dissemination or use of this information by a
person other than the intended recipient is unauthorized and may be
illegal.  Thank you."
*************************************************************

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2