It's funny you should bring up expiration dates on soldering materials,
I'm going through the same drill today with wire solder.
It's funny how different manufacturers put different shelf life dates on
their wire solder. I know that different flux types or alloys may come
into play when determining the shelf life, but it just doesn't make
sense to me.
For instance:
AMTECH NC-61 No-Clean wire solder, shelf life 12-months from date of
manufacture.
KESTER 44 Activated Rosin Cored solder, shelf life for alloys containing
>70% lead, the shelf life is two years from the date of manufacture.
Other alloys have a shelf life of three years.
MULTICORE 366 Flux, HMP, SN/PB/AG, shelf life minimum 5-years from date
of receipt (this according to a phone call I made this morning).
I'm getting ready to throw away about 30-rolls of solder...actually, I'm
going see if anybody here at work needs a roll or two first. But deep
down inside I know this solder is absolutely fine. Rules is rules
however...
-Steve Gregory-
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: Friday, February 09, 2007 10:09 AM
To: [log in to unmask]
Subject: Re: [TN] What to do with expired solder paste?
It seems to me you need to bring your storage and handling procedures
out of cold storage. Send the paste to Steve.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Friday, February 09, 2007 8:26 AM
To: [log in to unmask]
Subject: [TN] What to do with expired solder paste?
Was sorting through the fridge in the stockroom at work...pushed aside a
couple of sandwiches and yogurts (the stockroom people keep their
lunches in there...) and came across a box with 9kg(18 jars) of solder
paste expired in mid 2004 - a brand we don't use any more. Standard
63/37 no-clean.
What would you do with it? Never even been opened.
Genny.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|