That is correct.
Per Table 1 of ANSI/ESD S20.20, the minimum recommended technical range is <
1 x 10E9 ohms.
The exterior of most Metal In shielding bags <10E11 ohms. So it is not
proper ESD control to place the ESD Bag between the ESD sensitive items and
the ESD worksurface.
Gene Felder
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hogg, Blair K.
Sent: Monday, February 05, 2007 6:19 AM
To: [log in to unmask]
Subject: Re: [TN] ESD Question
Bogert,
The bag neither contributes to nor detracts from the ESD protection
while the assembly is at an ESD workstation and the operator is
grounded. The item should be placed into the bag before the operator
disconnects from the grounding system to leave the station, and should
not be removed from the bag until the operator has reconnected to the
grounding system.
Having the bag under the assembly during processing would most likely
violate good housekeeping practices at the workstation - if hand
soldering is being done the hot iron could touch the bag and melt it,
causing residue to accumulate on the tip. If assembly or test operations
are being performed the bag tends to get in the way.
Blair
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of - Bogert
Sent: Saturday, February 03, 2007 2:09 PM
To: [log in to unmask]
Subject: [TN] ESD Question
February 3, 2007
An OEM protects his circuit card assemblies by placing them in an ESD
bag when they are not being worked on or inspected. My question is if I
remove the assemblies and place them on top of the ESD bag which is
placed on the work surface of an ESD grounded work bench and am
connected to ground via the normal wrist strap, is there a concern if
the assembly is on the ESD bag surface versus the grounded work surface?
If so, what is? the reason?
Some folks have stated the item should not rest on the bag but I cannot
fina any ESD requirement in the 20.20 ESD spec that prohibits this.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
*******************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they
are addressed. If you have received this email in error please notify
the system manager.
This footnote also confirms that this email message has been swept
for the presence of computer viruses.
www.Hubbell.com - Hubbell Incorporated
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|