TECHNET Archives

February 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 5 Feb 2007 09:06:45 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Amol (349)" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Kane, Amol (349)" <[log in to unmask]>
Parts/Attachments:
text/plain (245 lines)
Dear all,

Since we are on the topic of conformal coating, I wanted to get a feel for how conformal coating masking requirements are being requested by the customer and being handled by the manufacturers. The customer drawing usually states the type of CC to be used and the keep-out areas for the coating (usually location Ids on the board). When one is masking on the keep-out areas, what tolerances are being used around the keep-out areas?.......IPC 610 D only states that there should be no CC on keep-out areas, and therefore by logical deduction, also assumes that all areas except the keep-out areas are to be covered by coating.

Obviously, there are practical limitations to this requirement. For example, a test via is a keep-out area, but the trace running from the via is not. Is everybody out there JUST masking the via, and then doing manual touch up on the extra keep-out area if any, afterwards? If one goes too close, the coating flows on the keep-out area, and if one leaves some space, you are violating IPC specs! .,..........I am thinking along the lines of asking customers to specify a tolerance for the keep-out areas as some of them are very particular about this issue.


Requesting your thoughts, current best practices etc

Regards,
Amol



 -----Original Message-----
From: 	TechNet [mailto:[log in to unmask]]  On Behalf Of Barmuta, Michael
Sent:	Friday, February 02, 2007 6:27 PM
To:	[log in to unmask]
Subject:	Re: [TN] Humiseal Masking Tape Residues/latex peelable

Hi Steve: Well let's think about this again. Some food for thought......

*	I assume your are using the HT500 tape. Have you tried a
different tape? In addition to the HT500 we also use Shercon's
"Conformal Coat" tape. It has a different backing and adhesive.
*	Possible compatibility issue with the soldermask? Have you tried
the HT tape on a different soldermask and a different lot of boards with
the same soldermask?
*	Possible flux or wash residue or moisture interactions? Are the
boards washed and thoroughly dried prior to CC? 
*	Are you absolutely sure that the masking tape was on the board
for only an hour?
*	Could the tape been applied to a hot board? Locking in the
adhesive?
*	Since the initial problem have you built some up "by the book".
Same problem?

					
	
Have a Good Weekend
	
Mike Barmuta



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, February 02, 2007 12:19 PM
To: [log in to unmask]
Subject: Re: [TN] Humiseal Masking Tape Residues/latex peelable

Hi Michael!

Believe it or not, it is adhesive. When we go to remove the residue,
it's real gummy and sticky...just like the tape adhesive. Take a look at
this picture:

http://stevezeva.homestead.com/files/Tape_Adhesive.jpg

It's a piece of the tape that I've taken and carefully scrapped at on
the sticky (adhesive) side until I've gotten to the carrier part of the
tape, and the carrier part of the tape is actually clear...it's the
adhesive that's tan. I looked at the MSDS and the tape is actually a
polyethyleneterephthalate film, and the adhesive is listed as a rubber
adhesive.

Like I said, I've never had this problem before.I used Humiseal tape
over at LaBarge while I was there, and switched our conformal coat area
over to the tape since I've been here at OAI. I've just now started
seeing the problem.

The tape doesn't stay on the board for more than 1-hour after spraying
before we remove it. The one weird thing that I am seeing is that I only
see the residues at places like in my first picture where we've masked
over PTH locations where the tape is completely on the PCB soldermask. I
don't see the residues on places where the tape is over the tin/lead
board finish, or metal (like the connector sheilds on press-fit
connectors.

-Steve Gregory- 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Barmuta, Michael
Sent: Friday, February 02, 2007 12:34 PM
To: [log in to unmask]
Subject: Re: [TN] Humiseal Masking Tape Residues/latex peelable

Steve: I would agree with Doug. By the appearance and color of the
residue it looks like the tape itself.

We are also using Humiseal's tape, in both strip and dot form. We have
not seen any issues with adhesive residue. One thing we monitor closely
is how long the tape is on the board after application. After
application we wait for two hours then remove the tape. Longer times can
cause release problems with the tape.


Hi Kenny: We used to use a liquid latex maskant but found it messy and
cumbersome to use. Have you considered preformed masking aids or tape?
Or is the design such that they won't work?
Check with Chemtronics they had a peelable latex product, Chemmask HV.
The rheology of the formulation was very good, preventing it from
flowing or spreading out after application.

	
Regards
	
Michael Barmuta
	
Staff Engineer
	
Fluke Corp.
	
Everett WA
	
425-446-6076

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, February 02, 2007 9:31 AM
To: [log in to unmask]
Subject: [TN] Humiseal Masking Tape Residues...

Hi All!
 
I have a conformal coat masking problem too along with KennyB. We're
getting residues from the Humiseal tape we're using when we remove the
tape.
 
We're coating the boards with 1B31, and we don't bake the boards with
the tape on. We take the tape off right after we spray the board. Check
out:
 
http://stevezeva.homestead.com/files/Tape_Residues.jpg
 
I've not had this problem with Humiseal tape before. Our customer is
rejecting the boards and it is quite time consuming to remove these
residues.
 
I've got a call into Humiseal to see if they can help. Do any of you use
any other tape for masking that doesn't leave residues?
 
Have a great Friday!
 
-Steve Gregory-

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

This message (including any attachments) contains confidential and/or
proprietary information intended only for the addressee.  
Any unauthorized disclosure, copying, distribution or reliance on the
contents of this information is strictly prohibited and may constitute a
violation of law.  If you are not the intended recipient, please notify
the sender immediately by responding to this e-mail, and delete the
message from your system.  If you have any questions about this e-mail
please notify the sender immediately. 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


This message (including any attachments) contains confidential 
and/or proprietary information intended only for the addressee.  
Any unauthorized disclosure, copying, distribution or reliance on 
the contents of this information is strictly prohibited and may 
constitute a violation of law.  If you are not the intended 
recipient, please notify the sender immediately by responding to 
this e-mail, and delete the message from your system.  If you 
have any questions about this e-mail please notify the sender 
immediately. 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------





CONFIDENTIALITY NOTICE: 
This e-mail, and any attachments, is for the sole use of the intended 
recipient(s) and may contain information that is confidential and 
protected from disclosure under the law. Any unauthorized review, use, 
disclosure, or distribution is prohibited. If you are not the intended 
recipient, please contact the sender by reply e-mail, and delete/destroy 
all copies of the original message and attachments. 
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2