TECHNET Archives

February 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 2 Feb 2007 17:43:02 +0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Lin Leo <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain; charset=big5
From:
Parts/Attachments:
text/plain (30 lines)
Hi,
   
  Recently, we have a defect for through hole un-fill in lead free wave soldering process.
   
  PCB board thickness: 94 mil
  PCB surface finish: OSP(For high temperature type)
  Wave soldering alloy material: Sn-Ag-Cu
   
  Any through hole size have the same defect.
   
  Does anyone understand how to overcome this defect or have related research for that?
   
  Best regards
   
  Leo

 ___________________________________________________ 
 您的生活即時通 - 溝通、娛樂、生活、工作一次搞定! 
 http://messenger.yahoo.com.tw/

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2