This might help.
http://www.smtinfo.net/docs/Electronic%20Production/9.htm
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of James Verrette
Sent: Wednesday, January 24, 2007 7:56 AM
To: [log in to unmask]
Subject: [TN] SnPb HASL min thickness
I remember reading here that you need at least 100 uin thickness of HASL
to adequately protect the copper pads. A fabricator is asking to allow
40uin minimum. If the boards are assembled within a couple days after
being received what minimum thickness would be adequate. Would the
result of too little HASL show up immediately at assembly with dewetting
of the solder joints or could it show up later as cracked or broken
solder joints? I am assuming both.
Jim Verrette
Electrical Engineer
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------