Hi again Bev,
Aluminum foil works fine with an IR light rework station because it is
reflective. It doesn't use hot air like other rework stations do, and
adjacent components don't see anywhere near the heat like hot air rework
stations. But if you have any worries, you can use aluminum foil to
sheild them.
I've never really measured adjacent components because the station has
only two non-contact thermocouples, and I use one on the part being
reworked, and the other for the PCB temperature at the rework site.
To be honest, I've never really worried about adjacent components. I
know they've never went to reflow temperature because you can see that
in the solder joints. So I can say with certainty that they've never
exceeded 183 C.
-Steve Gregory-
-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Thursday, January 18, 2007 7:48 AM
To: Steve Gregory; TechNet E-Mail Forum
Subject: RE: [TN] Rework of circuit packs with MSL Parts
Steve,
Again I was not explicit. Yes, of course I was not referring to the part
being taken off (it is tossed) or the part being put down (agree with
what you do). I am concerned about adjacent MSL parts.
How do you know that AL foil is good enough? How high do you let those
other thermocouples get?
Bev
RIM
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: January 18, 2007 8:45 AM
To: TechNet E-Mail Forum; Bev Christian
Subject: RE: [TN] Rework of circuit packs with MSL Parts
Mornin' Bev,
Most of the time the only time I'll dry (bake) a board before rework is
when the board is polyimide. I'm not usually worried about the component
because the one on the board is being replaced by a new one, and if the
new one is a MSD, it either has been kept in a dry cabinent if the
package has been opened or the package has been sealed. If I question
whether or not it has been exposed, I will dry it before rework.
The rework station I'm used to working with monitors temperature of the
part being reworked and PCB temperature adjacent to the rework area in
real-time during the rework cycle with non-contact thermocouples. If I'm
concerned about any part adjacent to the part being reworked, I simply
take a piece of aluminum foil and sheild the part. The rework station
uses IR light, so it's very easy to do...
Steve Gregory
(Trying to thaw out from all the ice we've had here lately)
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Thursday, January 18, 2007 7:23 AM
To: [log in to unmask]
Subject: [TN] Rework of circuit packs with MSL Parts
Technetters,
We have required that circuit packs that are going to be reworked to be
dried before rework. My questions to all of you are:
1) Do you require this for all your boards irrespective of what is on
them?
2) Do you dry it to the requirements of the most sensitive MSL
component?
3) Do you use thermocouples to see how hot the MSL components are going
to get from radiated, convected and transmitted heat?
40 If the latter, what is the maximum temperature you allow the nearest
MSL component to reach before you require a pre-dry?
Thanks in advance.
Bev
RIM
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|