In my experience, temporary masks are applied by the EMS.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Burtt, Nigel
Sent: Wednesday, January 03, 2007 10:44 AM
To: [log in to unmask]
Subject: Re: [TN] Temporary peelable solder masks
Peter,
I guess in part that is what I am asking. Do US assemblers
more commonly use the in-house/DIY approach rather than have the PCBs
supplied with the masking pre-applied to a supplied (gerber layer?)
pattern. Alternatively I know that some use masking that is removed by a
post-wave-solder cleaning process rather than peelable. Just surprised
that what our suppliers seem to think is not a big problem to provide as
a normal service is apparently not so readily available in USA... Or
maybe it just depends who you ask!
Cheers
Nigel Burtt
Production Engineering Manager
Dolby Laboratories, Inc. - European HQ
Email: mailto:[log in to unmask]
Tel: +44 (0)1793 842132 [direct line with voicemail]
Fax: +44 (0)1793 842101
-----Original Message-----
From: Peter Swanson [mailto:[log in to unmask]]
Sent: 03 January 2007 15:37
To: TechNet E-Mail Forum; Burtt, Nigel
Subject: RE: [TN] Temporary peelable solder masks
Nigel,
You rightly draw the distinction between a) the types of temporary masks
which are pre-applied by screen printing, usually by the pcb fabricator
and b) the temporary masks which are dispensed on by the guys doing the
assembly. They are different.
Whilst it is obviously desirable to have this job done by your fab guy,
as you pointed out, it isn't always straightforward. In particular, I
remember a few years back when the process window on the screenable
materials wasn't very wide, resulting in problems from under/over cure,
removal, etc. Maybe the formulations are more robust today.
It is possible to make the "in-house" dispensable types more appealing.
Dispensing can be by fairly inexpensive robotics. Curing can be quick by
heat or UV. Is this approach an option?
Regards,
Peter
--------------------------------------------------------
Peter Swanson [log in to unmask]
INTERTRONICS http://www.intertronics.co.uk
Tel: +44 1865 842842 Oxfordshire, England
INTERTRONICS is dedicated to providing quality material, consumable and
equipment solutions to the high technology, high performance assembly
industries, incorporating outstanding levels of technical support and
customer service.
Read our blog! http://www.intertronics.co.uk/blog/blog.htm
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of N Burtt
Sent: 03 January 2007 09:27
To: [log in to unmask]
Subject: [TN] Temporary peelable solder masks
I'm being told that these are not widely used in USA, the common types
used here in the UK (Peters and Electramask) not readily available, and
they create packaging and shipping problems... thus US PCB suppliers
reluctant to supply PCBs with peelable masking applied. Is this true?
Now they are by no means a perfect solution to protecting holes on a PCB
during wavesolder, but am not aware of another way of doing so in a
no-clean RoHS process if fixturing can't do it. What do US PCB
assemblers do if pre- applied peelable masking is really not viable?
Other ideas?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
-----------------------------------------
This message (including any attachments) may contain confidential
information intended for a specific individual and purpose. If you
are not the intended recipient, delete this message. If you are
not the intended recipient, disclosing, copying, distributing, or
taking any action based on this message is strictly prohibited.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|