TECHNET Archives

January 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Tue, 9 Jan 2007 12:44:56 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (185 lines)
You nailed right on the nuts, Bev.
All, whether you use a wash process or a no-clean process, you still
need make sure you perform some type of testing and cleanliness
verification. Initially it should be a full qualification, and
thereafter a daily verification, such as ROSE.
No-clean does not mean no potential problems, and just because you run
boards through a wash process does not necessarily mean they are "clean
enough" that no issues will ever arise. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Tuesday, January 09, 2007 11:12 AM
To: [log in to unmask]
Subject: Re: [TN] Cleaning

John,
Not if they do their homework and do the proper testing to show that the
tweak in reactivity won't put them on dangerous ground.  That is why
there are tests like copper mirror, halide ion, British corrosion test,
SIR and electrochemical migration.
Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: January 9, 2007 12:02 PM
To: [log in to unmask]
Subject: Re: [TN] Cleaning

That's what I was thinking Brian...................8-)

With the change to lead free and the various "wetting" issues a lot of
people are using a more active flux if only to make the joints "look"
more
like 63/37 and as a result are having to use cleaning systems to remove
the flux.

Of course the ones that do not remove the flux will find out eventually
why they should have done!!

John

 
 
John Burke
 
(408) 515 4992

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Tuesday, January 09, 2007 2:43 AM
To: [log in to unmask]
Subject: Re: [TN] Cleaning

Peter

I'd bet water will be >15% this time.

Brian

Peter Swanson wrote:
> Just a follow up from last week.
> 
> The SMART Group has conducted cleaning surveys in the past on their 
> website.
> 
> This survey was conducted in 2002 and received 79 votes cast:
> 1. No-Clean 61%
> 2. Nitrogen with No-Clean 14%
> 3. Water Wash 15%
> 4. Solvent Clean 6%
> 5. Semi Aqueous 4%
> 
> At that time, then, about 75% of the participants did not clean. The 
> geographic profile is unknown (as any visitor to the website can cast
a
> vote, anonymously), although I expect it was European biased. Five
years
> later, I would guess no-clean to be a bit more popular. We'll see, a
new
> cleaning survey has just gone up! 
> 
> Not rigorously scientific, of course, just an indication of industry 
> trends.
> 
> Regards,
> Peter
> --------------------------------------------------------
> Peter Swanson           [log in to unmask]
> INTERTRONICS                http://www.intertronics.co.uk
> Tel: +44 1865 842842                   Oxfordshire, England
> 
> INTERTRONICS is dedicated to providing quality material, consumable 
> and equipment solutions to the high technology, high performance 
> assembly industries, incorporating outstanding levels of technical 
> support and customer service.
> 
> Read our blog! http://www.intertronics.co.uk/blog/blog.htm
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To 
> unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------



---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2