TECHNET Archives

January 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 4 Jan 2007 07:41:11 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Barmuta, Michael" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="US-ASCII"
From:
"Barmuta, Michael" <[log in to unmask]>
Parts/Attachments:
text/plain (423 lines)
Graham: As an OEM that has built both bare boards and PCA's and used
temporary soldermask resist (TSR) for 30+ years, let me address a couple
of your questions.

*	Bare board fabricators do apply peelable TSR, however there is
not a large demand for it. So finding a shop that offers it may be a
little difficult.
There are two main types of peelable TSR, latex based and vinyl based.
Typically the fabricators apply the vinyl style. It is applied to the
board with a squeegee by printing thru a screen imaged with the features
open to where the mask is desired then baked to cure. 
It works well if applied correctly, cured correctly and the printed
feature has the right design/shape. If done improperly it is a mess.
Hard to remove, breaking into small pieces, very labor intensive for
removal.


*	If using a water soluble TSR use an unfilled version. Some TSR
manufacturers add fillers such as talc or silica  to there products to
enhance the printing or rheology characteristics. Unfortunately as you
found out it tends to clog filters, wear nozzles/pumps, settle in low
spots, etc. Unfilled TSR's do not have this problem there are 100%
soluble. As I said above we have used TSR for 30+ years in our aqueous
wash system and not had any problems with the equipment.

	

	
Regards
	
Michael Barmuta
	
Staff Engineer
	
Fluke Corp.
	
Everett WA
	
425-446-6076
	


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
Sent: Thursday, January 04, 2007 6:57 AM
To: [log in to unmask]
Subject: Re: [TN] Temporary peelable solder masks

Similar to Steve, our military stuff always gets cleaned.  But I did
build some class 3 stuff with no-clean - mainframe equipment
(commercial) - with a previous employer.  Your bank wants class 3
product and very high reliability, but at least you can count on them to
not use a hose to clean it off, and they keep the office
air-conditioned.  
Given that at this employer we do contract manufacturing, the
likelihood of convincing all customers to agree to no-clean flux is
fairly slim and so it's difficult to justify looking at the
qualification work.  We also have the issue of supporting build over
many years, which often forces buying "end of life" batches of parts -
which become more difficult to solder over time, so a fairly active flux
is required.

If I'm understanding Nigel's question properly, I'd never heard of a
PWB manufacturer pre-applying peelable solder mask - it's not something
I've ever come across as an option.  Does it work well?  How does the
PWB manufacturer apply it?  

We use the DIY version, we apply it just before wave soldering.  We
currently use the peelable stuff, we had used the water soluble but with
some production volume increases we were finding it clogged up the
filters in the cleaners too quickly.  

regards,

Graham Collins
Process Engineer, 
L-3 Communications Electronic Systems Inc.
Halifax
(902) 873-2000 ext 6215

>>> [log in to unmask] 01/04/07 10:23AM >>>
As a yank, at every place I've worked at over the last 19-years has
cleaned everything that's been built (aside from the small amount of
no-clean residues from hand soldered components done at the end of the
main assembly).

Products built range from military hi-rel applications to consumer
electronics (but haven't built any high volume stuff like cell phones,
that's all gone to China). Our customers just wanted things clean...

-Steve Gregory- 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Swanson
Sent: Thursday, January 04, 2007 4:43 AM
To: [log in to unmask] 
Subject: Re: [TN] Temporary peelable solder masks

Cleaning: 

My guesstimate is that the UK is 85%+ no-clean after either reflow or
wave solder. In the latter case, the liquid fluxes have very low
solids
content these days (~ 2%), therefore low residue.

Cleaning takes place in quite hi-rel applications, or before conformal
coating, although not always in that case either.

No-clean could even be higher than 85% - maybe we'll run a survey here
through the SMART Group to give a better picture.

I suspect that the TechNet and similar forums' membership are not
typical of the assembly industry as a whole. I think it is skewed
towards the hi-rel, more complicated or leading edge end of the
industry, where the issues are more complex and the outcomes more
critical. Therefore people need more help, are prepared and required
to
go more in-depth, and cover their behinds with extensive in-house
research and evaluations... and use other resources. Hence, I think
that
the percentage of TechNet members who post-solder clean is higher than
the USA market as a whole, or anywhere else. Just an impression.

I also suspect that the profile of electronics assembly in the two
markets are similar, although the US is larger or course - the UK no
longer has any high volume consumer electronics or mobile telephone
manufacture. We have also lost all the major EMS companies like
Celestica, Flextronics, Solectron, Jabil, etc all of whom used to have
big factories here - we have just a few stubs left. We have got a
bunch
of medium size EMS companies, automotive electronics, quite a lot of
defence and military, instrumentation, medical, telecom, et al. Maybe
the originator of this thread's company, Dolby, is a good example of
what we have - they make professional digital audio products here.
Nigel
is a buddy, by the way.

If you divvy the whole thing up by IPC Class I, II, III - I think the
percentages would be about the same here and there. Cleaning,
therefore,
is not necessarily a class issue!

Peter
--------------------------------------------------------
Peter Swanson           [log in to unmask] 
INTERTRONICS                http://www.intertronics.co.uk 
Tel: +44 1865 842842                   Oxfordshire, England

INTERTRONICS is dedicated to providing quality material, consumable
and
equipment solutions to the high technology, high performance assembly
industries, incorporating outstanding levels of technical support and
customer service.

Read our blog! http://www.intertronics.co.uk/blog/blog.htm 

-----Original Message-----
From: Dehoyos, Ramon [mailto:[log in to unmask]] 
Sent: 03 January 2007 18:26
To: TechNet E-Mail Forum; Peter Swanson
Subject: RE: [TN] Temporary peelable solder masks


      There is another option, use of Kapton dots of different sizes.
They peel off rather easily.   Peter, are you saying  that after
fluxing
in the wave solder there is no cleaning either? Or only after reflow?
	Regards,
	Ramon
	 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Swanson
Sent: Wednesday, January 03, 2007 11:40 AM
To: [log in to unmask] 
Subject: Re: [TN] Temporary peelable solder masks

>>>> If you are washing the board after soldering

I believe that this is quite possibly the bigger distinction between
the
UK (& Europe?) and US pcb assembly profiles. We have little or no
water
cleaning of fluxes after soldering any more. 

I think the ratio of SMT to through hole is certainly on a par between
the two. Maybe even higher here, certainly not lower.

Regards,
Peter
--------------------------------------------------------
Peter Swanson           [log in to unmask] 
INTERTRONICS                http://www.intertronics.co.uk 
Tel: +44 1865 842842                   Oxfordshire, England

INTERTRONICS is dedicated to providing quality material, consumable
and
equipment solutions to the high technology, high performance assembly
industries, incorporating outstanding levels of technical support and
customer service.

Read our blog! http://www.intertronics.co.uk/blog/blog.htm 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Barmuta, Michael
Sent: 03 January 2007 16:26
To: [log in to unmask] 
Subject: Re: [TN] Temporary peelable solder masks

Nigel: If you are washing the board after soldering I would recommend
using a water soluble mask. We have used the Lackwerke Peters GmbH
peelable vinyl mask in the past but have moved away from it.

Using water soluble mask eliminates the labor intensity of removing
the
peelable style mask. Also depending on how the peelable is used,
configured, applied and cured it doesn't always come off that easily.
This is not aimed at the Peters mask but to peelables in general.

We apply the temporary solder mask at the assembly level. Since we
wash
after soldering, water soluble masking materials are used. They are
applied by imaged screen printing, localized liquid dispensing or
taping
depending on board design and volume of product. Screen printing is
the
most prevalent approach.

I'm not sure why your board fabricator is hesitant to use the peelable
unless they are not set up for doing imaged screening. However it's
not
a big leap from doing permanent mask to doing temporary mask. Perhaps
they don't have enough customer requests for this to put in the
process.

I can understand why the fabricator may be hesitant to apply the water
soluble mask. If the boards are nor packaged and/or stored correctly
it
can start to breakdown and also stick or brick together.


	
Regards
	
Michael Barmuta
	
Staff engineer 
	
Fluke Corp.
	
Everett WA
	
425-446-6076



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Burtt, Nigel
Sent: Wednesday, January 03, 2007 7:44 AM
To: [log in to unmask] 
Subject: Re: [TN] Temporary peelable solder masks

Peter,
          I guess in part that is what I am asking. Do US assemblers
more commonly use the in-house/DIY approach rather than have the PCBs
supplied with the masking pre-applied to a supplied (gerber layer?)
pattern. Alternatively I know that some use masking that is removed by
a
post-wave-solder cleaning process rather than peelable. Just surprised
that what our suppliers seem to think is not a big problem to provide
as
a normal service is apparently not so readily available in USA... Or
maybe it just depends who you ask!

Cheers


Nigel Burtt
Production Engineering Manager
Dolby Laboratories, Inc. - European HQ
Email: mailto:[log in to unmask] 
Tel:     +44 (0)1793 842132 [direct line with voicemail] 
Fax:    +44 (0)1793 842101

 

-----Original Message-----
From: Peter Swanson [mailto:[log in to unmask]] 
Sent: 03 January 2007 15:37
To: TechNet E-Mail Forum; Burtt, Nigel
Subject: RE: [TN] Temporary peelable solder masks

Nigel,

You rightly draw the distinction between a) the types of temporary
masks
which are pre-applied by screen printing, usually by the pcb
fabricator
and b) the temporary masks which are dispensed on by the guys doing
the
assembly. They are different.

Whilst it is obviously desirable to have this job done by your fab
guy,
as you pointed out, it isn't always straightforward. In particular, I
remember a few years back when the process window on the screenable
materials wasn't very wide, resulting in problems from under/over
cure,
removal, etc. Maybe the formulations are more robust today.

It is possible to make the "in-house" dispensable types more
appealing.
Dispensing can be by fairly inexpensive robotics. Curing can be quick
by
heat or UV. Is this approach an option?

Regards,
Peter
--------------------------------------------------------
Peter Swanson           [log in to unmask] 
INTERTRONICS                http://www.intertronics.co.uk 
Tel: +44 1865 842842                   Oxfordshire, England

INTERTRONICS is dedicated to providing quality material, consumable
and
equipment solutions to the high technology, high performance assembly
industries, incorporating outstanding levels of technical support and
customer service.

Read our blog! http://www.intertronics.co.uk/blog/blog.htm 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of N Burtt
Sent: 03 January 2007 09:27
To: [log in to unmask] 
Subject: [TN] Temporary peelable solder masks

I'm being told that these are not widely used in USA, the common types
used here in the UK (Peters and Electramask) not readily available,
and
they create packaging and shipping problems... thus US PCB suppliers
reluctant to supply PCBs with peelable masking applied. Is this true?

Now they are by no means a perfect solution to protecting holes on a
PCB
during wavesolder, but am not aware of another way of doing so in a
no-clean RoHS process if fixturing can't do it. What do US PCB
assemblers do if pre- applied peelable masking is really not viable?
Other ideas?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives 
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives 
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


This message (including any attachments) contains confidential 
and/or proprietary information intended only for the addressee.  
Any unauthorized disclosure, copying, distribution or reliance on 
the contents of this information is strictly prohibited and may 
constitute a violation of law.  If you are not the intended 
recipient, please notify the sender immediately by responding to 
this e-mail, and delete the message from your system.  If you 
have any questions about this e-mail please notify the sender 
immediately. 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2