Looks like a double sided cap layer build, and the spots could well be inclusions in the prepreg layer or over-cured resin spots on the prepreg which have not flowed properly during the bonding stage.
I agree that a bare board reflow cycle will highlight any delamination issues, which may propagate further. However, I would run 2 cycles just to make sure that whatever it is, is inert.
Colin W.T. McVean M.Inst.C.T
Production Manager
Artetch Circuits Ltd
Direct Dial 01903 712926
Switch Board 01903 725365
www.artetch.co.uk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: 10 January 2007 14:06
To: [log in to unmask]
Subject: Re: [TN] PCB's: White spots
Mornin' Everybody!
Juan has sent me two pictures of the white spots he's seeing. They're at:
http://stevezeva.homestead.com/files/Spot_1.JPG
http://stevezeva.homestead.com/files/Spot_2.JPG
From what I'm seeing, I don't know if I'd worry about them that much...just as long as the board isn't covered with these spots. These look like bare boards that haven't had anything done to them yet. Am I correct?
You might take one the boards that you see the spots in and run it through a reflow oven under a soldering profile and see if the spots get any bigger. If they didn't, I probably wouldn't worry about them.
-Steve Gregory-
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Juan T. Marugán
Sent: Wednesday, January 10, 2007 6:07 AM
To: [log in to unmask]
Subject: [TN] PCB's: White spots
In some PCB's we have detected white spots. Although I think these spots are not due to a delamination and the boards should be acceptable, I'd like to have your assessment.
Thank you in advance,
Juan T. Marugán López
Production QA
Indra Sistemas SA - Madrid (SPAIN)
www.indra.es
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|