LEADFREE Archives

January 2007

Leadfree@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Tom Davenport <[log in to unmask]>
Reply To:
(Leadfree Electronics Assembly Forum)
Date:
Mon, 8 Jan 2007 17:13:22 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (193 lines)
Reuven,
I've read the specs but don't see the sections calling out CCC by China
labs?  Are you sure it's in there?

Best regards,

Tom Davenport

VP Quality, Reliability and Technology

Ramtron International Corporation

1-719-481-7139




-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Reuven Rokah
Sent: Monday, January 08, 2007 7:39 AM
To: [log in to unmask]
Subject: Re: [LF] China RoHS Clarification

You should read the China std's:

SJ/T11365-2006 Test Methods for restricted substances in EIP

And SJ11363-2006 Requirements for concentrations limits for certain
hazardous substances in EIPs.

And start to make dialog with Chinese Labs managers.

Best Regards
Reuven ROKAH
e mail: [log in to unmask]


-----Original Message-----
From: Tom Davenport [mailto:[log in to unmask]]
Sent: Monday, January 08, 2007 4:22 PM
To: (Leadfree Electronics Assembly Forum); Reuven Rokah
Subject: RE: [LF] China RoHS Clarification

Once again we see a similar statement below "All the products /
components
should have CCC by Chinese Lab."  Reuven, would you please state the
source
or reference for this statement.  Thank you.

Best regards,

Tom Davenport

VP Quality, Reliability and Technology

Ramtron International Corporation

1-719-481-7139



-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Reuven Rokah
Sent: Monday, January 08, 2007 4:57 AM
To: [log in to unmask]
Subject: Re: [LF] China RoHS Clarification

-	China RoHS is without exemption so EU RoHS is not enough.
-	The estimation for catalogue publishing is Q1 07 and one year
implementation.
-	EFUP for some products have the Chinese inputs such Telecom 50
years.
-	All the products / components should have CCC by Chinese Lab.


------------------------------------------------------------------------
-------------------------------------------------
This transmission and any files attached to it contains confidential
and/or proprietary information and is intended only for the named
recipient.
If you are not the intended recipient, you are hereby notified that any
re-transmission, dissemination, disclosure or copying of this
information is strictly prohibited.

------------------------------------------------------------------------
--------------------------------------------------
Best Regards
Reuven ROKAH
e mail: [log in to unmask]


-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of N Burtt
Sent: Monday, January 08, 2007 12:18 PM
To: [log in to unmask]
Subject: Re: [LF] China RoHS Clarification

Its seems safe to assume that if your products already fall under RoHS,
then
they will be within scope of China's version. However, until "The
Catalogue" is
published (we have been told Sept 2007) the scope is not fully defined
and
there are no exemptions yet.

Almost all RoHS product utilises one or more the exemptions already (eg
high
melting point SPb for CBGAs and for IC internal die attach, lead in
ceramic for
SMT resistors, network infrastructure, servers) - so you may be EU-RoHS
compliant but not China-RoHS compliant. Will anyone feel brave enough to
put
on the China "green E" products and thus provide a false 0% declaration
for all
6 substances on these by March 1 2007?

If I'm right then everyone needs to use the qualified "EFUP" marking (at
least
until the catalogue clarifies scope and any exemptions) and the number
to put
in the circle is important - how about we all agree to use the
"inifinity" symbol
until further notice?!

However, for products which are assemblies of many different components
and
hundreds of homogenous materials that appears to fall within scope,
getting
the required information from suppliers to accurately complete the
required "Hazardous Material and contents" declaration... and do so in
Chinese... will be no mean feat given how difficult it was to even get
just a
documented yes/no answer from many suppliers about RoHS.

Nigel Burtt
Dolby Labs Inc

------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------

------------------------------------------------------------------------
----
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
------------------------------------------------------------------------
----
---

----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---

-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------

ATOM RSS1 RSS2