If you go the route that Christopher suggested, you should first make sure that the Lead bearing BGA body can withstand LF temperatures. most lead bearing components are rated @ 220 deg C. I would do a SMT reflow at lead-free temps without the lead bearing BGAs and then use a rework station to put down the lead bearing BGAs later.
Amol
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Christopher Nash
Sent: Tuesday, January 30, 2007 1:28 PM
To: [log in to unmask]
Subject: Re: [TN] Leaded and unleaded BGAs
Darrel, you can use the leaded BGA's in you assemblies, however your builds
will not be ROHS compliant. If you choose to go this route you will need a
profile that allows for both the leaded and lead-free material to reflow.
You should be fine with using a lead-free profile with lead free
temperatures. The only thing to keep in mind is that you may experience an
increase in voiding. The Leaded solder balls will reflow before the
lead-free paste which may then cause an entrapment of the flux volatiles
from the lead-free solder paste. In other words, the flux will not be able
to outgas and be trapped in the solder joint. This may cause a reliability
concern that you may not want to take chances with. I hope this will help.
Christopher J. Nash
Mid-West Technical Support Engineer
Indium Corporation of America
www.indium.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Darrel Therriault
Sent: Tuesday, January 30, 2007 1:17 PM
To: [log in to unmask]
Subject: Re: [TN] Leaded and unleaded BGAs
Richard/Technet,
Sorry for the confusion and my improper use of terms.
What I intended to say was we have BGAs with Pb balls. I was wondering if
there was an accepted process to attach those on a board that has non-Pb
components by either reballing them with nonPb balls, using SRT rework or
some profile that might allow both Pb and nonPb components to be run at
the same time.
If there is no acceptable method, I either need to consume them in Pb
assemblies (non-RoHS) or take an E&O hit on the Pb components.
DJT
"Stadem, Richard D." <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
01/30/2007 09:48 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Stadem, Richard D." <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Leaded and unleaded BGAs
By leaded/non-leaded are you speaking of LGA arrays (leadless gate
arrays) or of BGAs with SAC alloy?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Darrel Therriault
Sent: Tuesday, January 30, 2007 10:20 AM
To: [log in to unmask]
Subject: [TN] Leaded and unleaded BGAs
Technetters,
Question for the process folks.............
We have leaded BGAs that we could use and still maintain 5/6 RoHS
compliance.
Does anyone have a process for attaching leaded and nonleaded
components?
Using SRT for the leaded parts or even reballing them with nonlead?
Is there an acceptable method for doing this or are they E & O
candidates?
Any info appreciated................DJT
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|