It depends! Only if you want it to solder easily. The explanation here is if the hole is located in a large section or on the edge of a large section, yes you need it. However, if your hole is located in a trace portion of the plane that sticks out from the plane and the trace is of "normal width" then probably not. You need to look at the location of the hole and determine if is located in a large bit of copper that will act as a heat sink or not.
Hope this helps.
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor G. Hernandez
Sent: Friday, January 26, 2007 11:15 AM
To: [log in to unmask]
Subject: Re: [TN] Assemble question
Do all Power plane termination in a PTH have to have a wagon wheel design?
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Friday, January 26, 2007 9:50 AM
To: [log in to unmask]
Subject: Re: [TN] Assemble question
Ramon,
It should be in the IPC-2221A, §9.1.3. I just looked and couldn't find the calculations that were in IPC-D275 which has been superseded by the 2221 and 2222 documents.
Basically you would want to have some number of "spokes" that would satisfy the current carrying needs of the signal based upon the foil thickness, spoke width and acceptable (expected) temperature rise during operation. This would be much like calculating the size of your signal or power traces. The most common form is four spokes. Check your board layout software. Our PADS Power PCB has these as default patterns available in the shape library.
One thing to consider is if you are using heavy weight copper foil, the amount of copper plated into the holes should be increased for the increased current presumably running through holes, especially vias. One solution is to allow all your vias to fill with solder, but this could a pain if you are hand soldering. Does anybody still do hand soldering for production <grin>?
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Friday, January 26, 2007 10:26 AM
To: [log in to unmask]
Subject: Re: [TN] Assemble question
Hi Phil:
Excellent input. Could you provide more info? If it is possible,
such as the diameter of the wheels and spokes. I am sure that it would
depend on the power through. Is there a guide line for the design
engineers?
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Friday, January 26, 2007 8:30 AM
To: [log in to unmask]
Subject: Re: [TN] Assemble question
Bill,
The boards you describe are very similar to many of our boards. If this
is an old design board it may be missing thermal reliefs (looks like a
wagon wheel) on each hole that is connected to large copper areas such
as ground or voltage planes. Without the thermal reliefs the copper
acts like a huge heat sink. With the thermal reliefs you get thermal
isolation from the large copper mass while maintaining the appropriate
current carrying capacity. IPC-2222 outlines the calculations for
correct size and number of the spokes. I had a hard time convincing
people here to use them, but once we did the assemblers were successful
in hand soldering these connections without preheating the boards or
using two soldering irons. The thermal reliefs also improved our
soldering on those boards going through wave solder.
I hope this helps. Good luck.
Phil Nutting
Design for Manufacturing Engineer
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bill Dworak
Sent: Thursday, January 25, 2007 3:01 PM
To: [log in to unmask]
Subject: [TN] Assemble question
I am in need of some help with regards to assemble. I am a PCB
manufacture and have built a group of boards for one of my accounts and
they are having issues assembling and have asked me for help on the
issues they are having.
The product is 4 layer board power and ground planes with 2 OZ copper
inner layers the outer layers are 5 OZ copper. What is happening is that
because of the construction of the board it is acting like a big heat
sink and this is where the problems are coming from. These are old
through hole designs they are assembling them by hand they are heating
the irons way up causing surface issues on the boards and in some cases
lifting of pads is resulting when extreme heat is applied they are
heating them up a lot because of all the copper and as I am being told
the solder is not melting the way that it should.
Any suggestions to make this a smooth build ?
Thank you.
Bill Dworak
This email is intended solely for use by the individual to which it is
addressed and may contain information that is privileged and/or exempt
from disclosure under applicable law.
It may also contain data subject to
the International Traffic in Arms Regulations or Export Administration
Regulations and cannot be distributed or copied to foreign nationals,
residing in the US or abroad without prior approval of the US Department
of State or appropriate export licensing authority. If the reader is not
the intended recipient you are hereby notified that any distribution or
copying of this communication is strictly prohibited. If you have
received this communication in error, please notify the sender by email
or collect call and delete or destroy all copies of this email and/or
any files attachments.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|