TECHNET Archives

January 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 25 Jan 2007 07:15:01 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Amol (349)" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Kane, Amol (349)" <[log in to unmask]>
Parts/Attachments:
text/plain (70 lines)
Hi Ken,
I have been asked this question before from our exempt and excluded customers. First thing I would do is ask if the part manufacturer has done any Sn whisker testing, and if yes, request for the results. From there you can take the help of the following to determine your risk:

JESD22A121.01: Measuring Whisker Growth on Tin and Tin Alloy Surface Finishes, and 
JESD201: Environmental Acceptance Requirements for Tin Whisker Susceptibility of Tin and Tin Alloy Surface Finishes; and 
JEDEC/IPC joint publication JP002: Current Tin Whiskers Theory and Mitigation Practices Guideline

On our end this was a joint exercise, with us, as the CM, and our customer. Now, the JESD201 does mention that high Sn alloys are not generally allowed for class 3 applications, but hopefully, the data you get from the component manufacturer will help to draw objective conclusions about the risk of Sn whiskers in your application.

Hope this helps,

Amol



 -----Original Message-----
From: 	TechNet [mailto:[log in to unmask]]  On Behalf Of Bloomquist, Ken
Sent:	Wednesday, January 24, 2007 1:25 PM
To:	[log in to unmask]
Subject:	[TN] Lead-Finish Question

Here's a question for all the high rel people out there. We've received
a couple of notifications from major component suppliers that they will
no longer supply the parts we need with a SnPb finish. Instead they are
only supplying them with "Matt (Matte) Tin" finish. They do not talk
about any under plating which would be desirable for minimizing tin
whiskers.

How are you people who build for DOD and medical handling these
situations? Am I being too sensitive about Matt Tim?

By the way these are single source and SMT parts.

Thanks in advance,

KennyB

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------





CONFIDENTIALITY NOTICE: 
This e-mail, and any attachments, is for the sole use of the intended 
recipient(s) and may contain information that is confidential and 
protected from disclosure under the law. Any unauthorized review, use, 
disclosure, or distribution is prohibited. If you are not the intended 
recipient, please contact the sender by reply e-mail, and delete/destroy 
all copies of the original message and attachments. 
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2