Vic6or,
I have an old EMMI. Never heard of using a Emission Microscope for
investigation of boards. I use it for semiconductor examinations
(recombination of minority/majority carriers=photon emission, for
example). If later versions of my HYPERVISION is adapted even for board
shortage tracking, I don't know, but I doubt. A new EMMI costs from
300,000 USD and up to no limit, depends on for what purpose it will be
used. In my case, the built-in probe station was extremly expensive, for
use as probing RF GaAs wafers and chips.
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor G. Hernandez
Sent: den 22 januari 2007 17:58
To: [log in to unmask]
Subject: [TN] EMMI Chamber
Fellow TechNetters,
Requesting for assistance in locating a vendor who sales the EMMI
chamber.
This instrument is more sensitive than conventional thermal imaging.
Instrument used to identify minute short in PCBA for troubleshooting
purposes.
Vic6or,
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|