Jon,
The only thing I could find is a reference in the SAE archives
(http://www.aepetsche.com/english/Resource-center/Technical-resources/SAE-ar
chives/ArchiveCommitteeNotes.pdf)
The abstract basically states that there is no established shelf life for
wire.
If your wire is oxidized at the cut end, try cutting off and discarding
about 6 inches of wire and rechecking the strands. Wire should be pretty
good forever.
Eric Kalgren
Electrical Engineer
Cobham Defense Electronic Systems
Continental Microwave Division
11 Continental Drive
Exeter, NH 03833 USA
Tel: 603-775-5200
Fax: 603-775-5201
E-mail:[log in to unmask]
Website: http://www.cobhamdes.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jon Roberts
Sent: Thursday, January 18, 2007 11:51 AM
To: [log in to unmask]
Subject: [TN] SELF LIFE OF STRANDED WIRE
Searching for data or information regarding process control to self life of
stranded wire (M22759/32). Wire is used for both soldering and crimping. We
are considering two years from Date of manufacturing (DOM) from vendor.
Problem being experience is discoloration (oxidation) of wire surface.
Considering also using solderablitity criteria to determine if wire is
suitable for
crimping. Any help or information is extremely welcomed.
Jon
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|