TECHNET Archives

January 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jon Roberts <[log in to unmask]>
Date:
Thu, 18 Jan 2007 12:26:40 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Frederick Miller <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="Windows-1252"
From:
Frederick Miller <[log in to unmask]>
Parts/Attachments:
text/plain (38 lines)
I would do a "dip and look" test to verify that the wire is wetting.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Jon Roberts
Sent: Thursday, January 18, 2007 11:51 AM
To: [log in to unmask]
Subject: [TN] SELF LIFE OF STRANDED WIRE


Searching for data or information regarding process control to self life of 
stranded wire (M22759/32). Wire is used for both soldering and crimping. We 
are considering two years from Date of manufacturing (DOM) from vendor.  
Problem being experience is discoloration (oxidation) of wire surface.  
Considering also using solderablitity criteria to determine if wire is suitable for 
crimping.  Any help or information is extremely welcomed.  

Jon

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2