TECHNET Archives

January 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Thu, 18 Jan 2007 08:13:17 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Nowland, Russell Howard (Russell)" <[log in to unmask]>
Subject:
From:
"Nowland, Russell Howard (Russell)" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (95 lines)
Hey Bev,

I hope you are doing well.  It depends on the repair method and whether
you want to save the components for FMA analysis.  If you are going to
using a repair system (e.g. AirVac SRT, etc..) that concentrate the heat
into the PWB (FR4 in our case) then yes, you need to bake or you could
get delamination, blistering, or noticeable physical change in the
PWB/soldermask.

Also, if you want to do FMA on the components, and you can't or don't
want to cut the leads off, you have to treat it like the MSD that it is
and bake appropriately.

If it is a small device that you can remove with hand tools (Metcal or
Hakko type) then you are not going to get the PWB hot and therefore you
do not need to bake.  I don't recommend using these tools if you want to
do FMA.

Call me on my cell if you want to talk directly.  I am south of the
border in Guadalajara for the next few weeks.

Take care,

Russell Nowland
Alcatel-Lucent           
Supply Base Engineer
Address: 14000 Quail Spring Parkway, Suite 300
Oklahoma City, OK 73134
email: [log in to unmask]
Desk: 405-302-1660
Cell: 405-203-0034
Fax: 405-302-1622
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Thursday, January 18, 2007 7:23 AM
To: [log in to unmask]
Subject: [TN] Rework of circuit packs with MSL Parts

Technetters,
We have required that circuit packs that are going to be reworked to be
dried before rework.  My questions to all of you are:
1) Do you require this for all your boards irrespective of what is on
them?
2) Do you dry it to the requirements of the most sensitive MSL
component?
3) Do you use thermocouples to see how hot the MSL components are going
to get from radiated, convected and transmitted heat?
40 If the latter, what is the maximum temperature you allow the nearest
MSL component to reach before you require a pre-dry?

Thanks in advance.

Bev
RIM



---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2