TECHNET Archives

January 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 16 Jan 2007 10:52:32 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Subject:
From:
Richard Kraszewski <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (183 lines)
I agree.  It more than likely is pronounced ROSS rather than "ROSE"  or
"row-has", as I was once corrected to this point by a Brit working in
the ministry in charge of RoHS in England. 

Rich K / GTS


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jeffrey Bush
Sent: Tuesday, January 16, 2007 11:18 AM
To: [log in to unmask]
Subject: Re: [TN] Best ROSE Tester

It all in the pronunciation - RoHS is pronounced like rose frequently
although the correct pronunciation is ROSS.  It is like arguing speeding
ticket and moving violation with a cop - both get you the same fine.

 

 

Jeffrey Bush

Director, Quality Assurance and Technical Support

VERMONT CIRCUITS INCORPORATED 

           76 Technology Drive - POB 1890 

              Brattleboro, Vermont 05302

                Voice - 802.257.4571 ext 37 

                    Fax - 802.257.0011

                       <http://www.vtcircuits.com/> 

________________________________

From: [log in to unmask] [mailto:[log in to unmask]] 
Sent: Tuesday, January 16, 2007 10:48 AM
To: Jeffrey Bush
Cc: [log in to unmask]
Subject: Re: [TN] Best ROSE Tester

 


FYI 

Niton sells RoHS testers not ROSE testers 



Joel Alexander

APSCO Quality Assurance Manager




Jeffrey Bush <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]> 

01/16/2007 10:02 AM 

Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Jeffrey Bush <[log in to unmask]>

To

[log in to unmask] 

cc

 

Subject

Re: [TN] Best ROSE Tester

 

 

 




http://www.niton.com/

Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED 
          76 Technology Drive - POB 1890 
             Brattleboro, Vermont 05302
               Voice - 802.257.4571 ext 37 
                   Fax - 802.257.0011
                      <http://www.vtcircuits.com/> 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bloomquist, Ken
Sent: Monday, January 15, 2007 1:17 PM
To: [log in to unmask]
Subject: [TN] Best ROSE Tester

I know there are several different brands of ROSE testers out there and
I would like to get some feedback on what experiences you've had with
the different brands, good and bad.

If you don't feel comfortable responding through TechNet you can reply
directly to me.

Thanks,

KennyB

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

ForwardSourceID:NT000AC042     


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2