Now there you have an intriguing question, if you don't get an answer call
me and I will arrange to go measure it.
The strength is to some extent going to be impacted by the solderable finish
and the shear speed.
Like I said, if you don't get an answer I will arrange to measure some for
you. My guess is going to be somewhere north of 2000 grams? Assuming
1000Grams per end.
Werner are you on line??
John
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Todd, Richard
Sent: Thursday, January 11, 2007 3:04 PM
To: [log in to unmask]
Subject: [TN] SMD Capacitor Shear Strength
I have a question for the oracle . . .
Does anyone know what is the solder joint shear strength for an 0603
capacitor (assuming standard eutectic solder)?
Regards,
Rick Todd
Senior Engineer
Process Quality Engineering
Panasonic Automotive Systems Company of America
Division of Panasonic Corporation of North America
776 Highway 74 South, Peachtree City, GA 30269
770-515-1087 Direct
678-458-2887 Cell
770-486-2248 Fax
[log in to unmask] <mailto:[log in to unmask]>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|