TECHNET Archives

January 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Peter Swanson <[log in to unmask]>
Date:
Wed, 3 Jan 2007 13:26:09 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
From:
"Dehoyos, Ramon" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (244 lines)
      There is another option, use of Kapton dots of different sizes.
They peel off rather easily.   Peter, are you saying  that after fluxing
in the wave solder there is no cleaning either? Or only after reflow?
	Regards,
	Ramon
	 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Swanson
Sent: Wednesday, January 03, 2007 11:40 AM
To: [log in to unmask]
Subject: Re: [TN] Temporary peelable solder masks

>>>> If you are washing the board after soldering

I believe that this is quite possibly the bigger distinction between the
UK (& Europe?) and US pcb assembly profiles. We have little or no water
cleaning of fluxes after soldering any more. 

I think the ratio of SMT to through hole is certainly on a par between
the two. Maybe even higher here, certainly not lower.

Regards,
Peter
--------------------------------------------------------
Peter Swanson           [log in to unmask]
INTERTRONICS                http://www.intertronics.co.uk
Tel: +44 1865 842842                   Oxfordshire, England

INTERTRONICS is dedicated to providing quality material, consumable and
equipment solutions to the high technology, high performance assembly
industries, incorporating outstanding levels of technical support and
customer service.

Read our blog! http://www.intertronics.co.uk/blog/blog.htm

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Barmuta, Michael
Sent: 03 January 2007 16:26
To: [log in to unmask]
Subject: Re: [TN] Temporary peelable solder masks

Nigel: If you are washing the board after soldering I would recommend
using a water soluble mask. We have used the Lackwerke Peters GmbH
peelable vinyl mask in the past but have moved away from it.

Using water soluble mask eliminates the labor intensity of removing the
peelable style mask. Also depending on how the peelable is used,
configured, applied and cured it doesn't always come off that easily.
This is not aimed at the Peters mask but to peelables in general.

We apply the temporary solder mask at the assembly level. Since we wash
after soldering, water soluble masking materials are used. They are
applied by imaged screen printing, localized liquid dispensing or taping
depending on board design and volume of product. Screen printing is the
most prevalent approach.

I'm not sure why your board fabricator is hesitant to use the peelable
unless they are not set up for doing imaged screening. However it's not
a big leap from doing permanent mask to doing temporary mask. Perhaps
they don't have enough customer requests for this to put in the process.

I can understand why the fabricator may be hesitant to apply the water
soluble mask. If the boards are nor packaged and/or stored correctly it
can start to breakdown and also stick or brick together.


	
Regards
	
Michael Barmuta
	
Staff engineer 
	
Fluke Corp.
	
Everett WA
	
425-446-6076



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Burtt, Nigel
Sent: Wednesday, January 03, 2007 7:44 AM
To: [log in to unmask]
Subject: Re: [TN] Temporary peelable solder masks

Peter,
          I guess in part that is what I am asking. Do US assemblers
more commonly use the in-house/DIY approach rather than have the PCBs
supplied with the masking pre-applied to a supplied (gerber layer?)
pattern. Alternatively I know that some use masking that is removed by a
post-wave-solder cleaning process rather than peelable. Just surprised
that what our suppliers seem to think is not a big problem to provide as
a normal service is apparently not so readily available in USA... Or
maybe it just depends who you ask!

Cheers


Nigel Burtt
Production Engineering Manager
Dolby Laboratories, Inc. - European HQ
Email: mailto:[log in to unmask] 
Tel:     +44 (0)1793 842132 [direct line with voicemail] 
Fax:    +44 (0)1793 842101

 

-----Original Message-----
From: Peter Swanson [mailto:[log in to unmask]]
Sent: 03 January 2007 15:37
To: TechNet E-Mail Forum; Burtt, Nigel
Subject: RE: [TN] Temporary peelable solder masks

Nigel,

You rightly draw the distinction between a) the types of temporary masks
which are pre-applied by screen printing, usually by the pcb fabricator
and b) the temporary masks which are dispensed on by the guys doing the
assembly. They are different.

Whilst it is obviously desirable to have this job done by your fab guy,
as you pointed out, it isn't always straightforward. In particular, I
remember a few years back when the process window on the screenable
materials wasn't very wide, resulting in problems from under/over cure,
removal, etc. Maybe the formulations are more robust today.

It is possible to make the "in-house" dispensable types more appealing.
Dispensing can be by fairly inexpensive robotics. Curing can be quick by
heat or UV. Is this approach an option?

Regards,
Peter
--------------------------------------------------------
Peter Swanson           [log in to unmask]
INTERTRONICS                http://www.intertronics.co.uk
Tel: +44 1865 842842                   Oxfordshire, England

INTERTRONICS is dedicated to providing quality material, consumable and
equipment solutions to the high technology, high performance assembly
industries, incorporating outstanding levels of technical support and
customer service.

Read our blog! http://www.intertronics.co.uk/blog/blog.htm

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of N Burtt
Sent: 03 January 2007 09:27
To: [log in to unmask]
Subject: [TN] Temporary peelable solder masks

I'm being told that these are not widely used in USA, the common types
used here in the UK (Peters and Electramask) not readily available, and
they create packaging and shipping problems... thus US PCB suppliers
reluctant to supply PCBs with peelable masking applied. Is this true?

Now they are by no means a perfect solution to protecting holes on a PCB
during wavesolder, but am not aware of another way of doing so in a
no-clean RoHS process if fixturing can't do it. What do US PCB
assemblers do if pre- applied peelable masking is really not viable?
Other ideas?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
-----------------------------------------
This message (including any attachments) may contain confidential
information intended for a specific individual and purpose.  If you are
not the intended recipient, delete this message.  If you are not the
intended recipient, disclosing, copying, distributing, or taking any
action based on this message is strictly prohibited.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

This message (including any attachments) contains confidential and/or
proprietary information intended only for the addressee.  
Any unauthorized disclosure, copying, distribution or reliance on the
contents of this information is strictly prohibited and may constitute a
violation of law.  If you are not the intended recipient, please notify
the sender immediately by responding to this e-mail, and delete the
message from your system.  If you have any questions about this e-mail
please notify the sender immediately. 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2