In a message dated 12/6/2006 3:48:59 P.M. Eastern Standard Time,
[log in to unmask] writes:
I got your pictures and put them in a *.doc file. They are here:
_http://stevezeva.homestead.com/files/Mask.doc_
(http://stevezeva.homestead.com/files/Mask.doc)
____________________________________
Eeek! That's certainly not orange-peel.
Are any of those boards already stuffed and, if-so, did they actually pass
cleanliness?
Pits like that love flux (and anything else that comes their way).
Buyer Beware...
ROBERT LAZZARA
VP, Business Development
T: (800) 560-9457
F: (800) 878-5566 (y servicio de mensaje espaņol)
E: [log in to unmask]
W:_ www.CircuitConnectUSA.com_ (http://www.circuitconnectusa.com/)
Circuit Connect, Inc.
ISO Certification : UL Listed : RoHS Exports : IPC Member : SMTA Member
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------