TECHNET Archives

December 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "West, Jim" <[log in to unmask]>
Date:
Thu, 28 Dec 2006 11:45:09 -0500
Reply-To:
Subject:
From:
Bill Kunkle <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (87 lines)
Jim,

Although your attachment does not travel thru Technet, I found that this
package is a QFN style component.

I suggest a stencil opening design as follows:
  perimeter leads: 1 mil width reduction, 100% length, 2 mil corner radii
  center lug: print 50 - 60% of the the metallized area

Use the area ratio calculation to insure good paste release.

This scheme works well for most QFN/MLF components.

Bill Kunkle
Manager of Stencil Technology
MET Assocs.
140 Mt Holly Bypass  Unit 10
Lumberton, NJ  08048

www.metassocs.com
Ph: 609 261 2670  Fx: 4007



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of West, Jim
Sent: Thursday, December 28, 2006 9:27 AM
To: [log in to unmask]
Subject: [TN] DRK package


Hi,

Looking for some help with the package shown within this email.  The
package virtually sits flush with the PCB, and the pads are directly
under the body of the part.  The pads are exposed on the side, but by a
very small amount.  I have a lot of questions regarding the processes
from the beginning to the end, but wanted to see if anyone else runs
this type of package and what your experiences have been like?  Some
questions would be stencil apertures design guideline, paste height,
after reflow inspection method, and reworking.

Best Regards,



Jim West
Engineering Manager
Nexergy Inc.
www.nexergy.com
tel: (614) 351-6216
fax: (614) 324-1979



This email message and all attachments transmitted with it are intended
solely for the use of the addressee(s) and may contain legally privileged,
protected or confidential information. If you believe that you have received
this message in error, please notify the sender immediately by email reply
and please delete this message from your computer and destroy any copies.

--------------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2