There is a recent paper by Craig Hillman etal. on Sn-Ag-Cu solder
accelerated life testing. Take a look at some of the data presented on SAC
vs. SnPb.
Paper title is:
Here is a brief excerpt from the results:
You can down load the paper from www.dfrsolutions.com
<http://www.dfrsolutions.com/>
pratap singh
____________________________________
Tel/Fax: 512-255-6820; Cell: 512-663-8903
www.rampinc.com ; EMail: [log in to unmask]
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------