Not exactly like that but I have seen strange corrosion under mask follow
via holes from one side of the board to another. The root cause was a
leaking battery. Something sort of Electrochemical action caused the
corrosion to migrate under the mask and generally not jump from one circuit
to another.
I wonder if the case instance of where it appears to jump from the plane to
the trace isn't in fact two cases one from the via in the plane and one from
the component through hole itself. C-35, was it removed? A failed
electrolytic cap?
What is the nasty brown near J11, component side.
On the solder source side near S21 switch 4, what is that big blob adjacent
to the land?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Monday, December 04, 2006 11:27 AM
To: [log in to unmask]
Subject: [TN] water water everywhere!
The following files show the two sides of a PCB in a professional weather
station. This shows four dark areas which the manufacturer has ascribed to
water penetration. These are centred on a hole. The whole thing seems funny
to me, as it has happened on only a few of the holes.
I understand that it was housed in a water-tight case, not very far from the
Pacific coast. I was not able to ascertain the laminate type, but it would
not surpise me if it were paper based (FR3?).
Has anyone seen anything like this?
Brian
http://www.realweatherstation.com/FILES/DSCN9441.JPG
http://www.realweatherstation.com/FILES/DSCN9440.JPG
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|