I'm no materials guy and I don't know if all inks are created equal in the
extent they bind up silver but in the experience I had it was the silver
that caused switch failure.
Hey, if I was an expert at anything why would I be a QE? Where else is a
recovering VW mechanic supposed to go looking for work? ;^)
Have you looked at an undisturbed suspect under high magnification? You see
any dendrites or resisdue of growth that's been powdered by key action?
I'd encourage you to set up a sample in a humidity chamber with keypad
voltage applied and watch what happens (visually and to
isolation/resistance between sides of the key switch).
dw
At 05:17 PM 12/17/2006, carl wrote:
>The ink is a heavy silver-fill with resistively less than 0.01 per square
>when dried. Is this something that I should worry about? If so, where can
>I find more information on the "migration risk" and how much to worry?
>
>Thanks,
>Carl
>
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Dwight Mattix
>Sent: Friday, December 15, 2006 6:43 PM
>To: [log in to unmask]
>Subject: Re: [TN] Membrane keypad failures
>
>Is there any silver content in the conductive ink? If below 100 ohms/sq then
>it probably has it intentionally and is a migration risk.
>
>There the risk of unintended silver in carbon ink as well. Long ago and far
>away i lived through an ugly humidity keypad field issue on a test
>deployment of wireless local loop phones in India. Finally discovered we
>were getting carbon ink that had residues of silver from previous mixes.
>You throw that silver into the mix with a phone operating with an
>continuously biased keypad, in a condensing monsoon environment in
>Bangalore, and voila! First failures came inside 30 days of fielding.
>
>Thank goodness for Bangalore traffic -- the test system installers were
>lucky to get around the city and install more than a couple phones/day.
>Most of the hardware was still on the shelf and we were able to recall and
>send reworked units to India and outfit a test system in Myanmar with
>properly reworked and re-qual'd units in the nick of time.
>
>The rework evolution and requal effort was a whole 'nother story involving
>walnut shells, lemon pledge and BB's -- takes at least 3 beers to tell it
>properly. Still have that qual plan around here somewhere...
>
>cheers,
>dw
>
>
>At 03:25 PM 12/15/2006, Carl VanWormer wrote:
> >
> >The dielectric is Electordag 452SS UV Curable Dielectric Coating. The
> >manufacturer says they coat with 2 layers to reduce the chances of a
> >pinhole opening allowing a short circuit. Is this a possible clue of
> >something to chase for my humidity related shorts?
> >
> >Carl Van Wormer
> >Cipher Systems
> >
> >-----Original Message-----
> >From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Lazzara
> >Sent: Thursday, December 14, 2006 6:08 AM
> >To: [log in to unmask]
> >Subject: Re: [TN] Membrane keypad failures
> >
> >[log in to unmask] writes:
> >
> >have two membrane keypads that have shown intermittent "short circuit"
> >failures.
> >Hello, Carl:
> >
> >OK, you've probably already looked for residual conductive ink between
> >conductors, but look closer for dust. Over-cured thick film conductive
> >polymers lose ductility and become [relatively] brittle. The
> >"...wiggling, banging..."
> >you described could produce enough conductive particulate between the
> >circuits to yield an intermittent high-resistance short.
> >
> >I'm also wondering about your dielectric: What is the dielectric
> >material (e.g., is it solder mask)?
> >
> >
> >ROBERT LAZZARA
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|