Excellent guess. Yes it does happen. But, more often in small holes. These
were pretty big.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hfjord
Sent: Friday, December 15, 2006 1:13 PM
To: [log in to unmask]
Subject: Re: [TN] How does this happen?
Mebbe gas bubbles? Such bubbles are sometimes hard to remove from small
spaces. We have seen plating with bubble problems, not boards, but maybe
boards can get into bubble-obstacles as well?
Inge
----- Original Message -----
From: "Steve Gregory" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, December 14, 2006 10:21 PM
Subject: [TN] How does this happen?
Hi all!
Well, the day is just about done here and boy am I glad...
We build a little board here (lots of them actually) that we call a "leaf
board" because of it's shape and small size. It has double-sided SMT on a
thin (.031"), immersion silver finished PCB. There are two PTH hall-effect
switches that we hand solder onto the board. We're using standard 63/37
solder BTW...
One of my operators stopped me to tell me that she was having a hard getting
good fillets on some of the switches on one of the panels she was working on
(they come in a 18-up panel). So I look at it and then tell her I see why
she's having trouble. Take a look at this picture and you'll see why she was
having trouble too:
http://stevezeva.homestead.com/files/Lovely_Barrels.jpg
So I tell her to give me the panel so that I can scrap the whole thing.
We aren't about to ship our customers something like that. I immeadiately
start looking at other WIP on the floor to see if I can find others that
have the same problem. I haven't found any as yet.
We emailed the photo to our fab vendor who immeadiately told us to ship back
all the bare boards that we have in our stockroom and they will screen them
for the problem. We've got a bunch in WIP right now that we have to look
closely at.
What actually causes something like that? The panel that we're working with
is only about 6" X 6", so I should expect that there's at least another half
dozen or so panels out there that might have this problem depending on how
big a panel the board house was building, right?
Further still, how does one panel get screwed-up like this and not the
others?
I'm ready to go home now...
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|