TECHNET Archives

December 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 8 Dec 2006 06:47:58 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Bloomquist, Ken" <[log in to unmask]>
Subject:
From:
"Bloomquist, Ken" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (61 lines)
Ingemar,

You bring up an interesting point. When I go through the list it sort of
reads like an economics chart. Lead, cheap, 5% recycle; Gold, valuable,
99% recycle.

Coincidence, I think not!

KennyB

-----Original Message-----
From: Ingemar Hernefjord (KC/EMW)
[mailto:[log in to unmask]] 
Sent: Friday, December 08, 2006 6:20 AM
To: [log in to unmask]
Subject: [TN] The 'poisonous'- computer reports
 
I doubt the results from these investigations. E.g. This  one: 

Lead 6.2988 3.8 5% Metal joining, radiation shield/CRT, PWB 

Is really 6.2 percent of a typical homeputer Lead? And is the recycling
of Lead only 5 % ??

Tin 1.0078 0.6 70% Metal joining/PWB, CRT 

Is Tin really only 1% of the computer weight while Lead is 6%, and why
is the recycling of Tin efficiency 70 % when  Lead is only 5% ?

Copper 6.9287 4.2 90%  Conductivity/CRT, PWB, connectors 

Same with Copper, which has 90% recycling efficiency.

Gold 0.0016 <0.1 99% Connectivity, conductivity/PWB, connectors 

And Gold with 99% recycling efficiency!!! 

I have a feeling, that such reports are 'one-eyed', am I thinking wrong?
(I wood nearly use the word 'manipulated', but hesitated...).  Is the
extremly low recycling efficiency of Lead the reason for banning Lead?
Or, vice versa, if Lead recycling efficiency had been same as for Tin,
then had Lead banning never been actual?

Not against the LF wave, but want know what is true and reliable.

http://www.sclf.ca/hazards.php


Inge
SMW

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2