As good as dipping is for applying conformal coating most conformal coating users spray it or use a Nordson select coat. Conformal coatings have a nasty habit of wicking up into places they shouldn't be (like connectors). Masking is time consuming and ill defined.
Spraying will not cover the back sides of the flat leads of ball grid arrays. In a perfect world the coating would provide a complete envelope over these leads, bridging the gaps between the leads. This doesn't always happen, particularly in the corners and particularly when a tall component blocks spray from one side. In this instance the complete envelope (or bag without a hole) is wishful thinking. Sometimes bridging of the coating between leads is iffy.
Liquid conformal coatings have a tendency to run off sharp bends in flat wire leads (we called those bends knees). These "knees" do not fluoresce when coated boards are inspected with a black light in a darkened room.
Doug Pauls' employer (and I'm sure some other companies) recognized the short comings of traditional conformal coatings for this application and developed their own techniques.
I have seen many instances where smaller companies try to develop similar solutions "on the fly" with unexpected and undesired consequences.
Edward Mines
---------------------------------
Sponsored Link
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Mortgage rates near 39yr lows. $420,000 Mortgage for $1,399/mo - Calculate new house payment
|
|
|