Making the CC viscosity at 30 seconds on #2 Zhan Cup will
eliminate the wicking up of unsealed leads in connectors or other parts.
The better way would be to design boards using only sealed lead parts,
then wicking up would not be an issue.
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas O. Pauls
Sent: Friday, December 01, 2006 3:10 PM
To: [log in to unmask]
Subject: Re: [TN] conformal coating as under fill
Mr. Stadem's comment about conformal coating wicking is true. I have
seen instances where it got inside connectors making them impossible to
connect or gluing them shut.
**Yup, we agree there.
The IPC should make recommendations regarding conformal coating
masking in their hand book. Should it be left on after coating? Subject
to qualification?
**If there was any recommendation, it should be to never leave tape on.
Too many tapes have too much crap in the adhesive to make it a long term
reliability material. Especially after you throw varying amounts of
solvent at it from the coating. What kind of tape you use for masking
depends on what materials you are using, whether you clean afterwards,
the end use environment, etc. Talk with your coating supplier to get
the right kind of masking tape for the coatings used and their
recommendations on how it should be used.
Mr. Stadem is mistaken regarding conformal coating and "moisture
condensation". Moisture yes, condensation no. A lot of other engineers
make this incorrect assumption. Conformal coating applied as liquid
doesn't provide water proofing on 3 dimensional objects. If it's
expected to then the qualifying tests should be changed.
**OK, now we have an argument, and it depends on how far you want to go
with the term "water proofing". In general, conformal coatings are
present to resist the flow of moisture and to prevent shorts from liquid
water contacting the energized assembly. No coating makes an assembly
truly water proof as all coatings have varying levels of water
permeability. We have applications here where assemblies are quite
likely to have liquid water running across them due to condensation in
the aircraft avionics bays. In that case, we might pick a silicone
coating and make sure that we have good coverage. In these
applications, conformal coat does provide protection on 3 dimensional
objects from liquid water. It all requires selecting the right material
and process.
Doug Pauls
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|