TECHNET Archives

December 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Date:
Mon, 18 Dec 2006 21:05:26 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Wenger, George M." <[log in to unmask]>
Parts/Attachments:
text/plain (174 lines)
I'll take a stab at answering the two questions you raise
Wayne,



I'll take a stab at answering the two questions you raised and also

correct one of the statements you made.



You indicated incorrectly that you "know that UL recently

"de-criminalized" ImAg, primarily based on IPC pressure."  The IPC

didn't pressure UL to "de-criminalize" immersion silver.  IPC member

companies who had experience with immersion silver surface finish on

PCBs jointed the IPC 3-11g sub-committee along with UL participation and

generated data that resulted in UL update the testing requirements that

were being imposed on silver finishes.  IPC and UL are organizations

that make specification changes based on data not pressure.  



As for why iNEMI hasn't "de-criminalized" there was no reason for them

to "de-criminalize" immersion silver because they had never

"criminalized" it.  If you look at the title of the paper written by the

iNEMI Tin Whisker User Group it covers "iNEMI Recommendations on

Lead-Free Finishes for Components Used in High-Reliability Products".

This group concentrated on component finishes not board finishes.  In

particular, if you look at Table 5 in their report that summarizes the

assessments of the individual members of the iNEMI Users Group relative

to PCB finishes you will see that there are no  tin whisker test

requirements for immersion silver.



As for papers on the electro-migration severity of immersion silver I

would start on the UL PCB site:

http://www.ul.com/pwb/silver.html



and then review the IPC 3-11g committee work.



Regards,

George

George M. Wenger

Andrew Corporation Wireless Network Solutions

Senior Principal FMA / Reliability Engineer

40 Technology Drive, Warren, NJ 07059

(908) 546-4531 [Office]  (732) 309-8964 [Cell]



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer

Sent: Monday, December 18, 2006 3:48 PM

To: [log in to unmask]

Subject: Re: [TN] iNEMI Hi rel Pb-free finish report



Sorry.  Here you go:



http://thor.inemi.org/webdownload/projects/ese/tin_whiskers/Pb-Free_Fini

shes_v4.pdf





Wayne



>>> [log in to unmask] 12/18/2006 2:57:21 pm >>>

Is the iNEMI 12/1/06 Pb-Free finish report published some

Wayne,



Is the iNEMI 12/1/06 Pb-Free finish report published somewhere?





Regards,

George

George M. Wenger

Senior Principle FMA / Reliability Engineer

Wireless network Solutions

Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908)

546-4531

[log in to unmask]





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer

Sent: Monday, December 18, 2006 2:50 PM

To: [log in to unmask]

Subject: [TN] iNEMI Hi rel Pb-free finish report



In this report (dated 12/1/06) there are several cautions about

Immersion Ag due to electro-migration issues, particularly in

sulfurous

environments.



I know that UL recently "de-criminalized" ImAg, primarily based on IPC

pressure.  Why hasn't iNEMI?



Can anybody recommend a paper which explains the severity of this

electro-migration issue with respect to ImAg?



Thanks,



Wayne Thayer



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt

or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16

for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------



------------------------------------------------------------------------

------------------------

This message is for the designated recipient only and may

contain privileged, proprietary, or otherwise private information.

If you have received it in error, please notify the sender

immediately and delete the original.  Any unauthorized use of

this email is prohibited.

------------------------------------------------------------------------

------------------------

[mf2]





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------





------------------------------------------------------------------------------------------------

This message is for the designated recipient only and may

contain privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender

immediately and delete the original.  Any unauthorized use of

this email is prohibited.

------------------------------------------------------------------------------------------------

[mf2]



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2