TECHNET Archives

December 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 14 Dec 2006 14:44:21 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Bev Christian <[log in to unmask]>
Parts/Attachments:
text/plain (142 lines)
Dave,
1) We test them as stand-alone, NOT in the presence of solder paste
2) They were cured by running them through a production reflow oven
first before testing
3) One supplier, who will remain nameless, has specifically told me they
do not test for SIR and ECM.  I am not sure about the others.

Bev
RIM


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: December 14, 2006 2:21 PM
To: [log in to unmask]
Subject: Re: [TN] Qualifying reworkable underfills

Hello Bev - see my comments below:

Dave Hillman
Rockwell Collins
[log in to unmask]




             Bev Christian
             <[log in to unmask]
             OM>
To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>
cc

 
Subject
             12/14/2006 12:50          [TN] Qualifying reworkable
             PM                        underfills


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
               Bev Christian
             <[log in to unmask]
                    OM>






Technetters,
Back after almost a year off-line.

*** Welcome back

It has always been my philosophy to thoroughly test ANY chemical that is
going to come in contact with a PCB or PCBA - tapes, labels, inks,
markers, adhesives, cleaners, temp solder masks, permanent solder masks,
flux stops, lubricants for compression fit pins, solder wicks, dusters,
freezing agents, OSPs, cored wires, fluxes, thinners, tacky fluxes,
paste fluxes, solder pastes, underfills, conformal coatings and thermal
compounds.

*** Good philosophy and are you sure that your list is complete? : -)

Lab testing includes copper mirror, halide ion, SIR and electrochemical
migration.  It sometimes includes other tests, but let's leave it at
this for the moment.

*** Wait a second - you didn't mention Ion Chromatography! You are going
to
make Mr. Pauls feel left out.

Here's my problem: I have tested many reworkable underfills from all the
people you can think of and I CAN'T FIND A SINGLE ONE THAT WILL PASS
BOTH IPC SIR AND ECM TESTING.  These materials were tested at the same
time that we had control coupons in the chamber (passed), solder pastes
(passed) and normal underfills (passed), so I doubt it was the chambers
(more than one) or that there were water droplets (checked, none
evident).

*** Ok , here is the only serious comment of the reply. Something
doesn't
make sense. The underfill materials surely meet the IPC SIR/ECM
requirements in a standard material test otherwise the suppliers would
not
market the underfill materials. So, my guess would be that possible root
cause for your reworkable underfill failures would either be improper
curing of the material (uncured underfill will not pass SIR/ECM) or
there
is a reworkable underfill/solderpaste flux incompatibility issue. Those
are the two items I would chase. Have you conducted IC testing on the
SIR/ECM coupons to see what extractable species are present?

My customers are pushing me to allow them to use the stuff and I am
resisting.  Comments, please.

*** You have three options:
-Resistance is futile, you will be assimilated.....
-Walk away from the light............
-Have the Technet crew give you suggestions

Bev Christian
RIM

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------



---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2