Yes. We did a lot of cross section without any abnormality.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Miguel Vallejo
Sent: Friday, December 01, 2006 1:08 AM
To: [log in to unmask]
Subject: Re: [TN] Solder Voids in Hole barrel after W/S
Irving,
Can you elaborate how you derived to the conclusion of having good hole wall quality? Assuming you've eliminated any other obvious anomaly that can cause outgasing, I would drill down on the copper plating concern. Have you had any cross-section done?
Miguel
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Irving Lee
Sent: Thursday, November 30, 2006 8:31 AM
To: [log in to unmask]
Subject: [TN] Solder Voids in Hole barrel after W/S
What are the critical control factors to avoid solder voids in hole barrel after W/S ?
We have checked following items , but still have serious solder void problem .
1. Good Hole Wall Quality
2. Good solderability for component tail 3. Good HASL thickness 4. No Ionic contamination
Irving Lee
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|