TECHNET Archives

December 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
[log in to unmask], TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 11 Dec 2006 16:03:37 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Thompson, David" <[log in to unmask]>
Subject:
From:
"Thompson, David" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (102 lines)
Joyce:  This report is one source stating the monochrome CRTs do not
fail TCLP and the arguments I have made.

In my experience, I have rarely seen references to phosphors as a source
of concern...its always lead, lead, lead.

Dave


-----Original Message-----
From: Joyce Koo [mailto:[log in to unmask]] 
Sent: Monday, December 11, 2006 1:56 PM
To: TechNet E-Mail Forum; Thompson, David
Subject: RE: [TN] The 'poisonous'- computer reports

wait. I thought it is the phosphor more so to cause problem...
http://www.ees.ufl.edu/homepp/townsend/Research/CRT/CRTDec99.pdf

           jk

abcd

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Thompson, David
Sent: Monday, December 11, 2006 10:52 AM
To: [log in to unmask]
Subject: Re: [TN] The 'poisonous'- computer reports


Glen / Ingemar:  CRTs do not contain layer of lead coating inside the
tube.  The lead is contained in the glass and is not readily
bioavailable in a landfill environment.

Today's computers probably do not contain 1/2 pound of lead.
Panasonic's current line up of laptops contain about 5 mg, a long way
from 1/2 pound.

David Thompson
Panasonic

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glen Herzog
Sent: Monday, December 11, 2006 10:15 AM
To: [log in to unmask]
Subject: Re: [TN] The 'poisonous'- computer reports

Ingemar,  possibly this article is suspicious because it was written in
1996, long before LCD screens and long before the introduction of RoHS &
WEEE.  CRTs have a heavy layer of lead in coating the inside of the
envelope.  I'll bet that todays lead weight in a desktop would not
exceed
1/2 pound.

Table presented in: Microelectronics and Computer Technology Corporation
(MCC). 1996. Electronics Industry Environmental Roadmap. Austin, TX:
MCC.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2