TECHNET Archives

December 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Sun, 10 Dec 2006 21:40:19 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=original
From:
Parts/Attachments:
text/plain (66 lines)
Sorry, you all, for bringing up an item too old. A disadvantage with letting
Internet files be on the web for 'ever' . All articles ought to have a well
visible cover  that tells 'this article is dated xxxxxx. Allright, the
notice was not quite in vain, a discussion about hundreds of tons of leaded
glass is still actual. Did not know that recycling such glass was a problem.
So called boemish crystal is a desirable group of finer stuff for elegant
dinner glasses or for prisms in big luxury lamps. Can't that kind of glass
industry take advantage of the abundance of leaded glass? On the other hand,
there will be inflation of boemish crystal, so it was perhaps not a good
idea. Wait, an other idea. Why not make a megalit, kind of  new Kaba stone
like the one in Mecca. A gigantic RoHs symbol. Hmm....end of good ideas.
Inge


----- Original Message -----
From: "Joe Fjelstad" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, December 11, 2006 8:41 PM
Subject: Re: [TN] The 'poisonous'- computer reports


> Hello Joyce,
>
> Thanks for the link.
>
> I could not find any statements about phosphor toxicity in the  reference.
>
> That aside, this might be the was the piece of work that caused  many to
> believe that lead was a leaching problem.
>
> As I understand it, the measurements were significantly off due to an
> unspecified experimental or arithmetic error which has since been
> admitted by the
> researchers.
>
> Someone else may have better insight.
>
> Very best,
> Joe
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2