Kerry-
Make sure you do elevated temperature accelerated aging of samples of
assemblies made with this alloy. I have had a few occasions where very
pretty "flowers" formed on points of devices in the vicinity of this
alloy. These are much bigger than whiskers, and may have to do with
small amounts of Pb getting into the system--however, I made every
attempt to keep the amount of Pb well below where I would normally
expect problems to develop.
Wayne
>>> [log in to unmask] 12/11/2006 10:01:06 am >>>
Hello esteemed Technet,
I am looking comments on what you would consider the advantages
and
disadvantages of this composition of this solder paste. (58Bi/42Sn)
Lower MP. 138 Degrees C.
Lower fatigue resistance
Wetting to ImAg??
Wetting to ImNiAu??
No Clean? Residue?
Intermetallic Formation?
Mixing with 63/37Sn?
Our application is an RF board where we would use this paste post Wave
/
Hand Solder.
Any comments appreciated.
Cheers,
Kerry
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|