Subject: | |
From: | |
Reply To: | |
Date: | Thu, 30 Nov 2006 09:08:00 -0800 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Irving,
Can you elaborate how you derived to the conclusion of having good hole wall
quality? Assuming you've eliminated any other obvious anomaly that can cause
outgasing, I would drill down on the copper plating concern. Have you had
any cross-section done?
Miguel
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Irving Lee
Sent: Thursday, November 30, 2006 8:31 AM
To: [log in to unmask]
Subject: [TN] Solder Voids in Hole barrel after W/S
What are the critical control factors to avoid solder voids in hole barrel
after W/S ?
We have checked following items , but still have serious solder void problem
.
1. Good Hole Wall Quality
2. Good solderability for component tail
3. Good HASL thickness
4. No Ionic contamination
Irving Lee
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|