Per IPC-4101B
/126
Tg = 170C
Td = 340C
T260 = 30 minutes
/129
Tg = 170C
Td = 340C
T260 = 30 minutes
At 07:49 AM 11/30/2006, you wrote:
>I haven't received my copy of 4101B yet so can someone tell me what
>/126 and /129 are
>
>Tg, Td, T260 etc,
>
>many thanks
>Geoff Layhe
>
>Private & Confidential:
>
>This e-mail message is confidential and is intended solely for the
>person or organisation to whom it is addressed. If the message is
>received by anyone other than the addressee please return the
>message to the sender by replying to it and then delete the message
>from your computer.
>
>
>
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
Donald Kyle C.I.D.+
Senior Development Technician
281-285-7528 voice
281-285-8593 fax
[log in to unmask]
Schlumberger
Sugar Land Product Center (SPC)
Mail Drop MD155-1
155 Industrial Boulevard
Sugar Land, Texas 77478
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|