You are correct.
My apologies, JaMi.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: Thursday, November 09, 2006 11:33 AM
To: [log in to unmask]
Subject: Re: [TN] Gold Embrittlement
Was that really necessary?
From my perspective, Jami's mistake was assuming Inge was using those
devices in a high-power application.
(and strong criticism of the work, but still informative)
Regardless, I thought the response was educational, and I'm glad I got
to read it.
Don't chase people away...
Jack
(p.s. I hope he IS willing to share more horror stories!)
Date: Wed, 8 Nov 2006 07:35:57 -0600
From: "Stadem, Richard D." <[log in to unmask]>
Subject: Re: Gold Embrittlement
MIME-Version: 1.0
Content-Type: text/plain; charset="us-ascii"
Content-Transfer-Encoding: quoted-printable
Perhaps you would be as willing and brave so as to post one of your own
ugly "curiosom aurorum" for us to pick apart for you.=20
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of JaMi Smith
Sent: Tuesday, November 07, 2006 5:45 PM
To: [log in to unmask]
Subject: Re: [TN] Gold Embrittlement
Inge ???
Not quite sure who this reply is from, or if this reply is directed at
me or not, or who 'Mr Besserwisser' or 'dear MR' are, but as for myself,
I simply responded to the pictures themselves (specifically the top
one), and the implied charge that all of this was due to gold
embittlement alone.
From my previous posts, you can see that I do not believe that gold
embrittlement alone is the culprit.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|