TGASIA Archives

November 2006

TGAsia@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Charlotte Hao <[log in to unmask]>
Reply To:
Asia Committe Task Group Forum <[log in to unmask]>, Charlotte Hao <[log in to unmask]>
Date:
Mon, 6 Nov 2006 01:09:22 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (38 lines)
 

Dear All,
 
Today there are 3 terms which are uncertain, pls give us your hand.
 
Thanks and regards 
 
Charlotte

 
 
Moisture Resistance                        防潮力             40.1925

The measure of how well the insulation characteristics of a material are maintained when exposed to temperature and humidity.

对材料暴露在温度湿度环境下良好地维持其原有绝缘特性的度量。

 

Muffle                                                 隔离罩             75.0780

An enclosure with a rectangular or oval cross-section that is located between the heating elements and the parts being processed that contains the atmosphere required for the reflow soldering process.

一个矩形或椭圆形的含有再流焊工艺所要求的气氛罩子,位于加热单元与被处理的部件之间。

 

Multilevel Experiment                      多重实验         91.0790

The evaluation of a small number of factors at a large number of levels.  

在多级别上对少数因子的评估。

 

 